Results 191 to 200 of about 10,603 (221)
Some of the next articles are maybe not open access.
Abstract This article reviews the historical development of fractography, from the early studies of fracture appearance dating back to the sixteenth century, and including the development of microfractography in the middle of the 20th century, to the current state-of-the-art work in electron fractography and quantitative fractography.
openaire +1 more source
openaire +1 more source
Fractography of self-glazed zirconia with improved reliability
, 2017Zhijian Shen +8 more
semanticscholar +1 more source
Failure Analysis of a GTD-111 Turbine Blade Using Metallurgical Analysis and Fractography
Journal of Failure Analysis and Prevention, 2019E. Poursaeidi +3 more
semanticscholar +1 more source