Results 161 to 170 of about 10,603 (221)
Some of the next articles are maybe not open access.

Formability and fractography of AA5754/polyethylene/AA5754 sandwich composites

Mechanics based design of structures and machines, 2020
Metal-polymer composites are one of the considered materials as a potential representative substitute for metals that have superior properties compared to monometallic materials.
F. Kazemi, R. Hashemi, S. Niknam
semanticscholar   +1 more source

Relationship between fractography, fractal analysis and crack branching

, 2020
A critical part of failure analysis is to understand the fracture process from initiation through crack propagation. Crack propagation in brittle materials can produce crack branching patterns that are fractal in nature, i.e., the crack branching ...
J. J. Mecholsky   +2 more
semanticscholar   +1 more source

Fractography off cast gypsum

Australian Dental Journal, 1982
AbstractA fractographical study of dental cast gypsum was made in order to correlate the mechanical properties with the microstructure. Wet specimens fractured under tensile stress showed intercrystalline fracture and the tensile strength depended on the porosity present.
T, Mori, M, Yamane
openaire   +2 more sources

Effect of Scan Direction on Tensile properties and Fractography of Laser Additive Manufactured Maraging Steel

Materials Today: Proceedings, 2019
Laser additive manufacturing (LAM) is the process used to fabricate near net shape from metallic powders. A major challenge with LAM fabricated parts is the materials performance to achieve required mechanical properties.
Tarun Bhardwaj, M. Shukla
semanticscholar   +1 more source

Fractography of Metals and Plastics

Practical Failure Analysis, 2001
Fractography is critical to failure analysis of metals and plastics. Fractography of plastics is a relatively new field with many similarities to metals. Using case histories, various aspects of failure analysis and fractography of metals and plastics are compared and contrasted. Failure modes common to both metals and plastics include ductile overload,
openaire   +1 more source

Fractography

2001
Abstract This article illustrates typical fractographic features for a number of different composite materials. It describes the differences in fracture characteristics due to different loading, material processing, and environmental conditions. The article presents fractographic data obtained from epoxy matrix materials.
openaire   +1 more source

Impact behavior and fractography of additively manufactured polymers: Laser sintering, multijet fusion, and hot lithography

Additive Manufacturing, 2019
To reduce the lead time, polymer fuel tanks could be toollessly produced using additive manufacturing (AM) technologies. Detailed knowledge of the performance of AM polymers is essential for the design and development of such components.
David Tasch   +3 more
semanticscholar   +1 more source

Fractals in fractography

Materials Science and Engineering, 1986
Abstract The fractal characteristics of a series of fractured AISI 4340 steel specimens were studied experimentally by means of vertical sections through the fracture surface. Extensive fractal data have been generated for both the fracture surfaces and their profiles.
Ervin E Underwood, Kingshuk Banerji
openaire   +1 more source

Failure analysis of a field brittle fracture composite insulator: Characterization by FTIR analysis and fractography

IEEE transactions on dielectrics and electrical insulation, 2018
A field brittle fracture composite insulator was examined and analyzed in detail in terms of chemical property and fractography with the purpose of obtaining the cause and mechanism of the failure as well as providing more detailed information on acid ...
Yanfeng Gao   +4 more
semanticscholar   +1 more source

Fractography of Weldments

Abstract This article provides an overview of fractography as it applies to metal weldments and presents examples of various fracture surface morphologies to demonstrate how fractographic analysis can be used to determine the cause of weld failures.
J.R. Stewart   +4 more
openaire   +1 more source