Results 11 to 20 of about 2,320 (181)
The reconstitution of the history of a fatigue process is based on the knowledge of any correspondences between the morphology of the crack surface and the velocity of the crack growth (crack growth rate - CGR).
Hynek Lauschmann +3 more
doaj +3 more sources
Creep rupture properties of bare and coated polycrystalline nickel-based superalloy Rene®80 [PDF]
The mechanism governing de-oxidation of vanadium metal is regarded as fundamental knowledge; however, it has not been elucidated in existing literature.
Barjesteh M.M. +3 more
doaj +1 more source
Optimization of T-6 cycle and Characterization of Si3N4 Reinforced High Strength Aluminum Metal Matrix Composites [PDF]
In this research, AA7068/Si3N4 composites were fabricated through stir casting with the attachment of ultrasonic treatment. The quenching medium and aging duration significantly influenced the hardness of Al alloy samples.
Ashish Kumar +3 more
doaj +1 more source
The purpose of this study was to understand the behavior of martensitic H13 steel in accordance with the microstructural evolution, mechanical properties and wear in repeated tempering cycles.
Amitkumar Shelar, B. P. Ronge
doaj +1 more source
Today’s demand for environmentally friendly and energy-efficient solutions to the construction industry has driven researchers to match natural resources with traditional technics to develop new building technologies.
F. P. Teixeira +3 more
doaj +1 more source
Effect of Boride Layer on PM HSS AISI M2 on the Mechanisms Acting in the Transverse Rupture Strength Test [PDF]
Herein, it was conducted a study in order to examine the main fracture characteristics in the transverse rupture strength test (TRS) of a high speed steel (HSS) AISI M2 produced by powder metallurgy (PM) and with boriding treatment.
Mateus Leal Arcego +3 more
doaj +2 more sources
The paper presents results of the investigations on the effect of the low-temperature thermomechanical treatment on the microstructure of AlZn6Mg0.8Zr alloy (7003 alloy) and the relationships between microstructure and fatigue properties and fractography
Aleksander Kowalski +4 more
doaj +1 more source
Cauchy-based Modelling in Cementitious Materials Technology [PDF]
Cauchy paved the way for constructing models in concrete technology, and elsewhere. He determined the (nonflat) surface area in 3D by measuring random total projections. Analogously, he determined the length of a curved line in 2D by way of measuring the
P. Stroeven, M. Słowik
doaj +1 more source
Axial fully-reversed strain-controlled (R=−1) fatigue experiments were performed to obtain data demonstrating the effects of building orientation (i.e. vertical versus horizontal) and heat treatment on the fatigue behavior of 17–4 PH stainless steel (SS)
Aref Yadollahi +3 more
doaj +1 more source
The microstructure and mechanical properties of Al2214-8 wt.% of 500 nm sized B4C particles reinforced composites were studied in this study. By using a liquid metallurgical process, composites containing 8 wt.% of B4C in Al2214 alloy were created.
Gopalan Kumar +3 more
doaj +1 more source