Results 101 to 110 of about 22,691 (145)
During the inertia friction welding (IFW) process of superalloy GH4169, the main mechanism for microstructural evolution is dynamic recrystallization (DRX).
Wei Xu, Li Wen Zhang, Chong Xiang Yue
core +1 more source
Effect of machining allowance on machining quality in honing nickel-base superalloy
For typical difficult-to-machine materials of nickel-base superalloy GH4169,honing experiments are carried out to study the hole surface roughness and cylindricity.Resultsshow that the surface roughness decreases gradually and tends to be stable as ...
DONG Hongliang +5 more
doaj
This paper utilized an in-situ electron microscopy technique along with high-temperature fatigue tests conducted at 298, 573, and 923 K to observe the initiation and propagation of short fatigue cracks (SFC) in the nickel-based superalloy GH4169 and to ...
Liu, Wenqi +7 more
core +1 more source
Numerical Simulation of Chip Formation in Metal Cutting Process
In order to study the chip formation mechanism in metal cutting process, based on finite element software ABAQUS, establish finite element model, and carry out numerical simulation on serrated chip formation of Ni-base superalloy GH4169 and ribbon chip ...
Yongjuan, ZHAO +2 more
core
This study takes large size samples after hot-upsetting as research objects and aims to investigate the optimization double-stage annealing parameters for improving the mechanical properties of hot-upsetting samples. The double-stage annealing treatments
Y C Lin, Ming-Song Chen, Guanqiang Wang
exaly +2 more sources
Some of the next articles are maybe not open access.
Related searches:
Related searches:
High temperature structure stability of GH4169 superalloy
Materials Science and Engineering: A, 2013Abstract The long-term thermal stability of GH4169 superalloy has been studied as a function of heat treatment and thermal exposure. The GH4169 superalloy was subjected to long-term unstressed heat treatment at 650 °C, from 200 to 1000 h. The microstructure, tension and stress rupture properties of the samples before and after long-term thermal ...
X.D. Lu, J.H. Du, Q. Deng
openaire +1 more source
Broaching Performance of Superalloy GH4169 Based on FEM
Journal of Materials Science & Technology, 2011The nickel-based superalloy GH4169 is an important material for high temperature applications in the aerospace industry. However, due to its poor machinability, GH4169 is hard to be cut and generates saw-tooth chips during high speed machining, which could significantly affect the dynamic cutting force, cutting temperature fluctuation, tool life, and ...
Xiangwei Kong +3 more
openaire +1 more source
Finite Element Modeling of the Linear Friction Welding of GH4169 Superalloy
Abstract In the present paper, finite element method (FEM) simulation of linear friction welding (LFW) GH4169 superalloy was carried out using ABAQUS software. The friction coefficients of GH4169 superalloy under different parameters (friction load, friction velocity and specimen temperature) were obtained using the friction and wear experiments.
Jinglong Li, Wenya Li, Xiawei Yang
exaly +2 more sources
Creep Deformation and Damage Characteristics of Nickel-Based Superalloy GH4169
Materials Science & Engineering A: Structural Materials: Properties, Microstructure and Processing, 2023Yingdong Song, Zhigang Sun, Xuming Niu
exaly +2 more sources
Study of Hot Deformation Behavior in GH4169 Superalloy
Advanced Materials Research, 2013In order to study the workability and optimize hot forming processing parameters for GH4169 superalloy, the hot deformation behaviors are investigated. The results show that the flow stress strongly depends on the strain rate, deformation temperature and strain.
Dong Xu Wen, Y.C. Lin, Ming Song Chen
openaire +1 more source