Results 111 to 120 of about 1,406,596 (298)
Mesoporous bioactive glass nanoparticles (MBGNs) are investigated for bone regeneration given their remarkable structural and functional properties. MBGNs are functionalized with Mn and Cu and incorporated with quercetin, a natural flavonoid exhibiting antioxidant, anti‐inflammatory, and antimicrobial properties.
Giovanni Lo Bello +5 more
wiley +1 more source
Comment on “Bioactive glass S53P4 vs. autologous bone graft for filling defects in patients with chronic osteomyelitis and infected non-unions – a single center experience” by Steinhausen et al. (2021) [PDF]
Martin McNally
openalex +1 more source
X‐Ray Tomography Analysis of Damage Mechanisms in Metal Matrix Syntactic Foams During Compression
In situ synchrotron X‐ray tomography is used to investigate the internal damage mechanisms of AlSi12 metal matrix syntactic foam with ceramic hollow spheres during compressive loading. It is concluded that a homogeneous distribution of the second‐phase filler material results in a sequential collapse in a localized region; this leads to controlled and ...
Indrajeet Tambe +8 more
wiley +1 more source
Thermodynamic Glass Transition in Finite Dimensions [PDF]
M. A. Moore, Joonhyun Yeo
openalex +1 more source
Failure mechanisms of kenaf/glass sandwich laminates subjected to low velocity impact loading
Seri Nur Zumaimi Ahmad Nadzri +5 more
openalex +1 more source
This study presents micropleated filters manufactured by needleless electrospinning. Nanofibers are deposited onto uniaxially pre‐stretched substrates that contract upon release, forming densely packed micropleats. This architecture increases effective surface area without enlarging the filter size, achieving quality factors comparable to those of ...
Aleksandr Fadeev +6 more
wiley +1 more source
Long fiber thermoplastic pellets of glass fiber/polypropylene from pultrusion process
Ponlapath Tipboonsri +2 more
openalex +1 more source
This study reports the fabrication of trabecular bioactive glass scaffolds (composition “1d”: 46.1SiO2‐28.7CaO‐8.8MgO‐6.2P2O5‐5.7CaF2‐4.5Na2O wt%) through vat photopolymerization and the relevant results from mechanical testing and in vivo implantation procedures in rabbit femora, showing great promise for bone tissue engineering applications.
Dilshat Tulyaganov +8 more
wiley +1 more source