Results 211 to 220 of about 3,654,663 (338)

Subgrain and Cavity Development during Creep of Al‐3.85%Mg

open access: yesAdvanced Engineering Materials, EarlyView.
Al‐3.85%Mg does form subgrains if crept at very high strains. This fact allows the unification of the creep description in two different alloys such as pure Al and Al–Mg alloys. It is classically considered that the creep mechanisms for type M (e.g., pure Al) and type A alloys (e.g., Al–Mg alloys) are different.
Augusta Isaac   +6 more
wiley   +1 more source

First‐Principles Modeling of Solid Solution Softening and Hardening Effects in Al–Mg–Zr–Si Aluminum Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
The role of various alloying elements in face‐centered cubic aluminum on the barrier of a Shockley partial dislocation during its motion is presented. The study aims to understand how alloying atoms such as Mg, Si, and Zr affect the energy landscape for dislocation motion, thus influencing the solid solution hardening and softening in aluminum, which ...
Inna Plyushchay   +3 more
wiley   +1 more source

Editorial: Coarse Graining in Quantum Gravity: Bridging the Gap Between Microscopic Models and Spacetime-Physics

open access: yesFrontiers in Physics, 2021
Astrid Eichhorn   +3 more
doaj   +1 more source

Microstructural Evolution and Mechanical Property Degradation of Sn0.5Ag0.7Cu5Bi Solder Joints with High Indium Alloying

open access: yesAdvanced Engineering Materials, EarlyView.
This study identifies 12 wt% indium (In) as the optimal composition for Sn0.5Ag0.7Cu5Bi solder joints, achieving 87% ductile fracture and 81% suppression of intermetallic compound (IMC) growth versus 4 wt% In. High‐In alloys (15–17 wt%) show abnormal IMC thickening due to thermal activation.
Liuwei Wang   +11 more
wiley   +1 more source