Results 191 to 200 of about 1,282,251 (292)

High‐Entropy Ti, Zr, Hf, Ta Multiphase Diboride with Deformation Resistance up to 2000 °C

open access: yesAdvanced Engineering Materials, EarlyView.
Ceramics are brittle and strength decreases with temperature. The multiphase high‐entropy (Ti0.25Ta0.25Hf0.25Zr0.25)B2 with heterogeneity at the nano‐ and microscale demonstrates deformation resistance up to 2000 °C, with maximum bending strength at 1800 °C.
Petre Badica   +3 more
wiley   +1 more source

Kidney volume measurement and predictive modeling in children aged 0-18 years using a computer-assisted surgery system. [PDF]

open access: yesSci Rep
Liu Y   +11 more
europepmc   +1 more source

Design and Evaluation of 3D‐Printed Polylactic Acid Composites Reinforced with Biodegradable Bamboo Powder and Jute Powder

open access: yesAdvanced Engineering Materials, EarlyView.
The study investigates 3D‐printed polylactic acid (PLA) composites with biodegradable bamboo and jute powder fillers. Mechanical, thermal, structural properties, and rheological behavior are discussed to evaluate composite performance. Morphological characterization indicates uniform dispersion and adhesion of the fillers in the PLA matrix with the ...
Vimukthi Dananjaya   +4 more
wiley   +1 more source

A Study on Thermal Expansion and Thermomechanical Behavior of Composite Metal Foams

open access: yesAdvanced Engineering Materials, EarlyView.
The coefficient of thermal expansion of steel–steel composite metal foam (S‐S CMF) is shown to be lower than that of bulk stainless steel while its performance under compression demonstrate excellent mechanical stability and strength at all temperatures with gradualsoftening from 400 to 600 °C.
Zubin Chacko   +2 more
wiley   +1 more source

Microstructure, Mechanical Properties, and Antibacterial Performance of Novel Fe‐Mn‐Zn Nanocrystalline Alloys Produced by Mechanical Alloying

open access: yesAdvanced Engineering Materials, EarlyView.
This article presents the development of Fe‐Mn‐Zn nanocrystalline alloys (0–9 wt% Zn) by mechanical alloying and subsequently hot pressing. Their microstructure, density, hardness, wear resistance, corrosion behavior, and antibacterial properties are systematically examined.
Ilker Emin Dag   +3 more
wiley   +1 more source