Results 1 to 10 of about 253,481 (293)
Investigation of residual stress changes and formation of hydride phase in production stages of Zr-1%Nb alloy [PDF]
Zr-1%Nb alloy is the most common alloy used as nuclear fuel cladding in Russian reactors. In producing a nuclear fuel cladding, the cold rolling (pilger) and the final straightening lead to the creation of residual stresses and a change in the ...
S.A. Miresmaeili Hafdani +2 more
doaj +1 more source
Hydride Conductivity in Nitride Hydrides [PDF]
13 pages, 6 ...
Andrew J. E. Rowberg +1 more
openaire +2 more sources
Simulation method for secondary hydriding breakage of zirconium alloy cladding
BackgroundWhen the fuel zirconium cladding tube of pressurized water reactor (PWR) breaks, the water flowing into the cladding will flash into water vapor under the action of the pressure difference between the inner and outer surface.
MA Yan, ZHANG Zhixin, CHEN Jiawei
doaj +1 more source
Transition metal-based materials and their catalytic influence on MgH2 hydrogen storage: A review
The dependence on fossil fuels for energy has culminated in its gradual depletion and this has generated the need to seek alternative source that will be environmentally friendly and sustainable.
Oluwashina Philips Gbenebor +1 more
doaj +1 more source
Interstellar hydrides—that is, molecules containing a single heavy element atom with one or more hydrogen atoms—were among the first molecules detected outside the solar system. They lie at the root of interstellar chemistry, being among the first species to form in initially atomic gas, along with molecular hydrogen and its associated ions.
Gerin, Maryvonne +2 more
openaire +6 more sources
A decanuclear silver chalcogenide cluster, [Ag10(Se){Se2P(OiPr)2}8] (2) was isolated from a hydride-encapsulated silver diisopropyl diselenophosphates, [Ag7(H){Se2P(OiPr)2}6], under thermal condition. The time-dependent NMR spectroscopy showed that 2 was
Yu-Jie Zhong +4 more
doaj +1 more source
Hydrogen Embrittlement Failure Behavior of Fatigue-Damaged Welded TC4 Alloy Joints
The interaction between fatigue damage and hydrogen in TC4 welded joints was analyzed considering specimens with different pre-cycles. The fracture failure caused by hydrogen-induced fatigue damage was investigated using tensile testing and ...
Xudong Feng +3 more
doaj +1 more source
Investigation of Magnetocaloric Properties in the TbCo2-H System
In this work the magnetocaloric effect in the TbCo2-H system in the region of the Curie temperature was studied both by direct and indirect methods in external magnetic fields up to ~1.4 and 14 T, respectively.
Galina Politova +6 more
doaj +1 more source
Hydride Reduction by a Sodium Hydride–Iodide Composite [PDF]
AbstractSodium hydride (NaH) is widely used as a Brønsted base in chemical synthesis and reacts with various Brønsted acids, whereas it rarely behaves as a reducing reagent through delivery of the hydride to polar π electrophiles. This study presents a series of reduction reactions of nitriles, amides, and imines as enabled by NaH in the presence of ...
Too, Pei Chui +4 more
openaire +4 more sources
Hydrogen Kinetics and Hydride Formation Effect on Zr-1Nb and Zr-1Nb-1Sn-0.1Fe Alloys for Nuclear Application [PDF]
The purpose of this study was to investigate the kinetics of hydrogen absorption and hydride formation and their effect on the mechanical properties in Zr-1Nb and Zr-1Nb-1Sn-0.1Fe alloys, which were thermomechanically processed and gaseously hydrided at ...
Leandro Martins de Oliveira +3 more
doaj +1 more source