Results 51 to 60 of about 513,634 (215)
The weak interlaminar properties severely hinder the high-property applications of carbon fiber (CF) reinforced thermoplastic composites. Here, interlaminar properties were significantly enhanced by introducing carbon nanotube (CNT) decorated polyether ...
Xukang Wang +6 more
doaj +1 more source
A multifunctional structural power composite is developed by integrating high‐mass‐loading Zn‐ion hybrid supercapacitors with metal mesh current collectors and aramid nanofiber‐based composite electrolytes, enabling simultaneous load‐bearing capability and enhanced areal energy storage.
Yuseung Choi +8 more
wiley +1 more source
Interlaminar fracture toughness of some polymer blends reinforced by fiber glass
The interlaminar fracture toughness of polymer blends reinforced by glass fiber has been investigated. Epoxy (EP), unsaturated polyester(UPE), polystyrene (PS), polyurethane (PU) and their blends with different ratios (10%PS/90%EP), (20%PS/80%EP), (20 ...
Harith I. Jaafer
doaj
INTERLAMINAR FRACTURE TOUGHNESS OF FIBER METAL LAMINATES
The aim of this paper is to investigate the feasibility of applying different DCB models to predict interlaminar toughness of composite laminates and FMLs and compare with experimental results.
Carlos Rubio-Gonzalez +2 more
openaire +1 more source
This study combines full‐field tomography with diffraction mapping to quantify radial (ε002$\varepsilon _{002}$) and axial (ε100$\varepsilon _{100}$) lattice strain in wrinkled carbon‐fiber specimens for the first time. Radial microstrain gradients (−14.5 µεMPa$\varepsilon \mathrm{MPa}$−1) are found to signal damage‐prone zones ahead of failure, which ...
Hoang Minh Luong +7 more
wiley +1 more source
Effects of stitching on delamination of satin weave carbon-epoxy laminates under mode I, mode II and mixed-mode I/II loadings [PDF]
The objective of the present study is to characterize the effect of modified chain stitching on the delamination growth under mixed-mode I/II loading conditions.
Trabelsi, Walid +2 more
core +1 more source
FE modeling of delamination growth in interlaminar fracture specimens
Interlaminar fracture specimens like Double Cantilever Beam (DCB), End Notched Flexural (ENF), Single Leg Bending (SLB) etc. are widely used for studying the interlaminar toughness of composite laminates. The aim of this paper is to analysis delamination
Vyacheslav Burlayenko, Tomasz Sadowski
doaj +1 more source
DYNAMIC INTERLAMINAR FRACTURE TOUGHNESS IN POLYMERIC COMPOSITES
A modified ENF specimens with off mid-plane delamination precrack was used to determine the mixed mode dynamic interlaminar fracture toughness of fiber composites at high crack propagation speeds. A strip of FM-73 adhesive film was placed ahead of the tip of the delamination crack created during laminate lay-up to increase the crack initiation ...
C. T. Sun, J.L. Tsai
openaire +2 more sources
This study investigates the effects of nano carboxylic acrylonitrile butadiene rubber (CNBR-NP) and nano acrylonitrile butadiene rubber (NBR-NP) on the interlaminar shear strength and fracture toughness of carbon fibre reinforced polymer composites (CFRP)
N. G. Ozdemir +5 more
doaj +1 more source
This review examines vitrimer performance from a broader perspective, considering not only dynamic covalent chemistry but also molecular structure, network architecture, and rheological behavior. These factors are discussed in relation to service and processing windows, reprocessing, repair, and engineering applications, providing a multiscale ...
Kyosun Ku, Hyeonuk Yeo
wiley +1 more source