Results 191 to 200 of about 2,276,316 (288)

Inflammatory Response‐Inspired Thermochromic Shield for Pneumatic Structures

open access: yesAdvanced Engineering Materials, EarlyView.
A thermochromic shield for pneumatic structures is developed, using anhydrous sodium acetate powder and thermochromic pigment‐included solution. In this shield composed of three layers, the exothermic and thermochromic reactions, followed by the mixture of both components, occur promptly with an incident of penetrating damage as a sign of initial ...
Hyun Jae Lee, Ryuma Niiyama
wiley   +1 more source

Sustainable Synthesis of Bio‐Based Magnetic and Conductive Wood for Electromagnetic Interference Shielding Applications

open access: yesAdvanced Engineering Materials, EarlyView.
A wood‐based magnetic and conductive material called Magwood (MW), capable of blocking almost 99.99% of electromagnetic waves (in the X‐band frequency range), is synthesized using a simple, solvent‐free process. MW is lightweight, resists water, and is flame‐retardant, making it a promising alternative for shielding electronics. The rapid proliferation
Akash Madhav Gondaliya   +3 more
wiley   +1 more source

Thermoelectric Modules Incorporating MgAgSb and Mg3(Sb,Bi)2 Synthesized Using a Melting Method

open access: yesAdvanced Engineering Materials, EarlyView.
A scalable synthesis method for a thermoelectric material of MgAgSb is established. A thermoelectric power module of MgAgSb/Mg3(Sb,Bi)2 is fabricated, showing the conversion efficiency of 7.4% at ΔT = 315 K. The performance is comparable to conventional Bi2Te3 modules when they are operated with an air‐cooled heat exchanger.
Kazuo Nagase   +8 more
wiley   +1 more source

Four‐Point Bending Tests at High Temperatures on Commercial MgO‐C Refractory Bricks with and Without Recyclate Considering Different Carbon Contents

open access: yesAdvanced Engineering Materials, EarlyView.
Four‐point bending tests are conducted in an argon atmosphere on commercial MgO‐C brick grades with and without MgO‐C recyclate from room temperature up to 1300 °C. No detrimental effect of the MgO‐C recyclates on bending strength is found. Instead, a decisive influence of the total carbon content is observed, with lower total carbon contents ...
Alexander Schramm   +5 more
wiley   +1 more source