Results 61 to 70 of about 2,759,057 (174)
Hot cracking and joint softening are the two main factors restricting the achievement of high-performance fusion welding joints of 7075 aluminum alloy. This paper utilized low heat input laser-melt inert gas welding (MIG) hybrid welding to butt weld 7075
Weiqing LIU +6 more
doaj +1 more source
Desenvolvimentos no processo híbrido Plasma-Mig para operações de soldagem e brasagem [PDF]
Tese (doutorado) - Universidade Federal de Santa Catarina, Centro Tecnológico. Programa de Pós-Graduação em Engenharia Mecânica.Avanços no desenvolvimento da tecnologia da soldagem têm ocorrido pela associação de dois processos, formando uma nova ...
Oliveira, Moisés Alves de
core
Analysis of Weld Formation Mechanism and Weld Pool Dynamic during Moving Laser-MIG Hybrid Welding
In order to better understand heat transfer and fluid flow pattern in the weld pool of laser-metal inert gas (MIG) hybrid welding aluminum-alloy process, weld formation mechanism and weld pool dynamic behavior were analyzed by a three-dimensional ...
Zhi Guo Gao
core +1 more source
Parameter Influence in CO2-laser/MIG Hybrid Welding [Elektronisk resurs]
Hybrid welding, as the combination of laser beam and arc welding, is an innovative joining technology that has many advantages compared to the single processes.
Heimbs, Sebastian, +3 more
core
Prospecções da natureza física da soldagem MIG automática de ligas de alumínuio [PDF]
Dissertação (mestrado) - Universidade Federal de Santa Catarina, Centro Tecnológico, Programa de Pós-Graduação em Engenharia Mecânica, Florianópolis, 2013Como processo de fabricação, a soldagem tem um papel de destaque dentro dos setores naval e ...
Marques, Cleber
core
Hybrid laser-MIG/MAG welding at ISI
Laser welds usually suffer from underfill defects because the welding is usually made without a filler wire. During the hybrid laser-MIG/MAG welding, the laser beam forms the melt pool, and the arc simultaneously delivers melted filler wire. The synergic
Mrňa, Libor
core
Crack propagation behavior of laser-MIG hybrid welded joints in 6005 aluminum alloy
The fatigue crack propagation behavior of laser-MIG hybrid welded joints in 6005A-T6 aluminum alloy is studied. Digital image correlation (DIC) technology is employed to capture the local displacement field near the crack tip during testing, enabling a ...
Ke LYU +5 more
doaj +1 more source
Achieving aerospace standard porosity levels when welding thin and thick-section aluminium using fibre-delivered lasers : executive summary [PDF]
Environmental and commercial pressures have forced the aerospace industry to look at alternatives to riveting for the manufacture of aluminium aircraft structures.
Verhaeghe, Ing G.
core
Hybrid laser-MIG welding : an investigation of geometrical considerations
Godkänd; 2005; 20061213 (haneit)
openaire +1 more source
Hybrid laser-MIG welding of steels for the energy industry
Laser-MIG welding can lead to the heterogeneity in the weld metal. A weld root's chemical composition corresponds to the base metal, while the face is formed dominantly by the filler wire that can have a different chemical composition.
Mrňa, Libor
core