Corrosion Behavior of Steels in Lead-Bismuth Eutectic: In Stagnant LBE Test at Low Oxygen Partial Pressure

12th International Conference on Nuclear Engineering, Volume 1, 2004
Corrosion test of three chromium-molybdenum steels — 2.25Cr-1Mo, Mod.9Cr-1Mo and 12Cr-steel (ASME P122) — has been performed in stagnant lead–bismuth eutectic (LBE) at low oxygen partial pressure at 550 °C up to 2,000 hours. After the test, the specimens were metallurgically examined using a scanning electron microscopy.
Tomohiro Furukawa   +2 more
openaire   +1 more source

Spectroscopic and microscopic study of the corrosion of iron–silicon steel by lead–bismuth eutectic (LBE) at elevated temperatures

Journal of Nuclear Materials, 2006
Abstract The performance of iron–silica alloys with different silicon composition was evaluated after exposure to an isothermal bath of lead–bismuth eutectic (LBE). Four alloys were evaluated: pure iron, Fe–1.24%Si, Fe–2.55%Si and Fe–3.82%Si. The samples were exposed to LBE in a dynamic corrosion cell for periods from 700 to 1000 h at a temperature ...
Allen L. Johnson   +7 more
openaire   +1 more source

Revealing wear mechanisms of coated shafts in low-speed journal bearings immersed in liquid Lead-Bismuth Eutectic (LBE)

Tribology International
This study investigates wear mechanisms of coated shafts in journal bearings within liquid lead-bismuth eutectic. Shafts were coated with TiAlN, a-C:H, multi-layer TiAlN with sputtered carbon, and chrome plating. Bearings made from sintered iron with carbon inclusions (DEVA 120 and DEVA 121) were tested in LBE at 200 °C and 50 rpm using a dedicated ...
Serag, Essam Sadik Talaat   +4 more
openaire   +1 more source

Effect of Temperature on Fretting Wear and Corrosion of 316L Stainless Steel In the Liquid Lead-Bismuth Eutectic (LBE)

Volume 3: Fluid-Structure Interaction; High Pressure Technology
Abstract The change of temperature in liquid lead-bismuth eutectic(LBE) can lead to the formation of oxide film with different properties on the surface of structural steel. In the lead-cooled fast reactor, the heat transfer tubes are the important place for heat exchange in the steam generator.
Hui Chen   +3 more
openaire   +1 more source

Investigation on fretting wear mechanism of 316 stainless steel induced by Ni dissolution during pre-immersion corrosion in the liquid lead-bismuth eutectic (LBE)

Tribology International, 2022
K. Hua   +9 more
semanticscholar   +1 more source

Investigation of the Corrosion of Steel by Lead-Bismuth Eutectic (LBE) Using Scanning Electron Microscopy and X-Ray Photoelectron Spectroscopy

2002
Lead Bismuth Eutectic (LBE) has been proposed for use in programs for accelerator transmutation of waste. LBE is the leading candidate material as a spallation target and an option for the sub-critical blanket coolant. The corrosion of 316 and 316L stainless steels by LBE has been studied using UNLV 's facilities for Scanning Electron Microscopy (SEM ...