Results 181 to 190 of about 646,440 (257)
Building machine‐readable vocabularies for materials science is slow, expert‐driven work. This study benchmarks 13 large language models on two of its first steps: finding candidate terms in engineering articles and deciding where they belong in a class hierarchy.
Thomas Bjarsch +3 more
wiley +1 more source
From hepatitis A to acute liver failure in a resource-limited setting: a case report. [PDF]
Dorante ICP +9 more
europepmc +1 more source
The temperature dependence of fatigue behavior in nickel‐based superalloys is investigated through high‐resolution measurements of plastic localization. While increasing temperature reduces localization and enhances fatigue performance in René 88DT, Inconel 718 exhibits a sharp degradation at intermediate temperature due to intensified slip ...
M. Calvat +5 more
wiley +1 more source
Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik +7 more
wiley +1 more source
Statin-Induced Hyper-Acute Reversible Liver Failure: A Case Report. [PDF]
AlTurki AA +4 more
europepmc +1 more source
The present study investigates recycling of NiTi shape memory alloys via vacuum induction melting. An ingot was synthesized from elemental Ni and Ti and subjected to three subsequent remelting cycles. Remelting increases process durations and impurity levels and adversely affects microstructures and functional properties.
Sakia Sophia Noorzayee +7 more
wiley +1 more source
Acute-on-chronic liver failure and immune dysregulation: Systemic inflammation and immunoparesis paradox. [PDF]
Drago AA +8 more
europepmc +1 more source
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar +7 more
wiley +1 more source
The incidence, frequency of late liver-related complications, and transplant likelihood in pediatric acute liver failure in Californian children. [PDF]
Lee JTC +11 more
europepmc +1 more source