Results 171 to 180 of about 28,440,571 (273)
Objective This study synthesized the content and reporting completeness of published physical therapist–led interventions for glenohumeral osteoarthritis (GHOA). Methods This systematic review undertook electronic database searches in PubMed, EMBASE, Cochrane, CINAHL, and PEDro (until June 2025) for any peer‐reviewed articles or studies describing ...
Daha G. Muhammad +5 more
wiley +1 more source
Objective Patient‐reported outcome measures (PROMs) are central to assessing symptom burden and treatment response in Osteoarthritis (OA) but are often embedded in unstructured clinical notes. We evaluated whether prompt‐engineered large language models (LLMs) could accurately extract or infer pain scores on a 0‐10 scale from routine OA clinical ...
Jainesh Doshi +7 more
wiley +1 more source
Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar +2 more
wiley +1 more source
Thermomechanical fatigue tests of laser beam powder bed fusion (PBF‐LB) Inconel 718 show that the additively manufactured material reaches almost the lifetimes of conventionally‐rolled material under no‐dwell conditions. Introducing dwell times at the maximum temperature markedly reduces the lifetimes due to pronounced grain boundary sliding associated
Stefan Guth +6 more
wiley +1 more source
Mass density governs the protective behavior of oxide layers on nuclear fuel cladding. Ptychographic X‐ray computed tomography measures zirconium oxide grown on Zircaloy‐4 under reactor and autoclave conditions, revealing nearly identical bulk densities of 5.1 ± 0.80 g cm−3.
Okan Yetik +9 more
wiley +1 more source
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar +7 more
wiley +1 more source
Comparison of Triply Periodic Minimal Surface Energy Absorbers Under Uniaxial Compressive Loading
This study investigates LCD 3D printed Triply Periodic Minimal Surface (TPMS) structures as mechanical energy absorbers. By comparing various base designs and layered combinations under uniaxial compression, it identifies that a Diamond‐Gyroid sandwich structure offers superior performance.
Sergej Grednev +2 more
wiley +1 more source
Experiments and thermophysical simulations were conducted to investigate the electron beam powder bed fusion electron beam (PBF‐EB/M) process for the γ′‐strengthened nickel‐based superalloy Inconel 738LC. The results demonstrate the impact of process‐induced microstructural variations on high‐temperature mechanical behavior, providing a basis for ...
Jan Niklas Petenati +11 more
wiley +1 more source
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas