Results 41 to 50 of about 21,417,156 (279)
To address the fracture control problem of X80 unequal-diameter tee used in China-Russia Eastern Gas Pipeline under low temperature environment (-45 ℃), the finite element model for X80 unequal-diameter tee with defects was built taking into ...
Zeguang YOU +3 more
doaj +1 more source
Influence of Temperature on Impact Toughness of HSLA Steels [PDF]
The aim of this paper is to present the influence of differ-ent temperatures on the impact toughness of welded joint of high strength low-alloy steel. The results of impact tests for all three constituents of the manual arc welded joint of NN-70 steel at
Bulatović, Srđan +2 more
core +1 more source
Influence of equal-channel angular extrusion on impact toughness of aluminum and brass at room and low temperatures [PDF]
Abstract Background Equal-channel angular extrusion is a severe plastic deformation process that can be used for grain refinement to improve material properties of bulk metals. In this paper, the effect of equal-channel angular extrusion on the impact toughness of aluminum 1100 and brass C26000 was investigated.
Wang, Jyhwen +3 more
openaire +1 more source
A simplified thermoplastic pultrusion model is developed to predict thermal fields in glass fiber/polyethylene terephthalate (GF/PET) composites with reduced computational cost. By combining effective material homogenization, validation against literature data, and Gaussian‐process‐based optimization, the study reveals how heating limits, pulling speed,
Elder Soares +3 more
wiley +1 more source
Effect of temperature on impact toughness of nuclear grade low-carbon tubular steel
In this study, the low-temperature impact toughness and tensile properties of nuclear grade low carbon tubular steel were systematically studied. A comparative discussion was conducted on the quantitative relationships between temperature and impact ...
Dongsheng Li +3 more
doaj +1 more source
The influence of centerline segregation on the low-temperature impact toughness of the heat-affected zone (HAZ) of welded joints was studied by welding experiments on X70 steel plates rolled from continuous casting slabs with segregation grades of class ...
Fujian Guo +4 more
doaj +1 more source
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar +7 more
wiley +1 more source
The possibility for the National Institute for Standards and Technology (NIST) to certify Charpy reference specimens for testing at room temperature (21 C 1 C) instead of _40 C was investigated in a previous study, in which a slightly increased ...
Lucon, Enrico ; Santoyo, Ray L.
core +2 more sources
Postbuild annealing systematically modifies the phase fractions and morphology of EB‐PBF processed Mo–9Si–8B. Quantitative microstructure–property correlations reveal how controlled phase evolution enhances high‐temperature compressive strength and creep resistance.
Christopher Schmidt +5 more
wiley +1 more source
HEA interlayers offer a versatile route for joining high‐performance structural materials. Their compositional and structural design regulates interfacial reactions, suppresses brittle IMCs, and improves metallurgical bonding. Sandwich interlayers further integrate defect healing with precipitation strengthening, enabling improved strength–ductility ...
Lin Yuan +4 more
wiley +1 more source

