Results 31 to 40 of about 20,057 (255)
A simplified thermoplastic pultrusion model is developed to predict thermal fields in glass fiber/polyethylene terephthalate (GF/PET) composites with reduced computational cost. By combining effective material homogenization, validation against literature data, and Gaussian‐process‐based optimization, the study reveals how heating limits, pulling speed,
Elder Soares +3 more
wiley +1 more source
To address the fracture control problem of X80 unequal-diameter tee used in China-Russia Eastern Gas Pipeline under low temperature environment (-45 ℃), the finite element model for X80 unequal-diameter tee with defects was built taking into ...
Zeguang YOU +3 more
doaj +1 more source
Phase Field Failure Modeling: Brittle‐Ductile Dual‐Phase Microstructures under Compressive Loading
The approach by Amor and the approach by Miehe and Zhang for asymmetric damage behavior in the phase field method for fracture are compared regarding their fitness for microcrack‐based failure modeling. The comparison is performed for the case of a dual‐phase microstructure with a brittle and a ductile constituent.
Jakob Huber, Jan Torgersen, Ewald Werner
wiley +1 more source
The effect of quenching cooling method on the mechanical properties of 20Cr1Mo1VTiB steel bar after overall heat treatment was studied through microstructure test methods such as mechanical property test, scanning electron microscope (SEM), transmission ...
Gong Xueting +3 more
doaj
Karl Popper and the Mechanisms of Hydrogen Embrittlement
Representation of the beginning of loss of ductility rather than embrittlement. Small concentrations of hydrogen in a diffusible form within iron are well‐established to harm the mechanical integrity of steels. There are theories that attempt to explain the pernicious role of hydrogen.
H. K. D. H. Bhadeshia
wiley +1 more source
The optimal aging temperatures of 400–550 °C for high strength steels falls into the dangerous temperature range of temper-embrittlement. To obtain a good low-temperature toughness, temperatures above 600 °C are usually selected for aging treatments ...
Xinghao Wei +7 more
doaj +1 more source
Low temperature impact toughness of structural steel welds with different welding processes
Influence of welding process and welding consumable on the impact toughness at low temperatures of the Heat Affected Zone (HAZ) and the weld metal in a structural steel weldment was investigated. A comparison of the low temperature impact toughness was made between the welded joints fabricated by Shielded Metal Arc Welding (SMAW) and Flux Cored Arc ...
Hyun-Seop Shin +4 more
openaire +1 more source
A two‐dimensional multiscale finite element analysis framework was established for the first‐generation MoSiBTiC alloy, and the mechanical and fracture‐related parameters of the constituent phases were calibrated through experiments and simulations. The framework provides a basis for analyzing crack propagation behavior in its complex microstructure ...
Junfeng Du +4 more
wiley +1 more source
This article uses scanning electron microscopy (SEM) and electron back-scattering diffraction (EBSD) to study the effect of C and Mn segregation on the microstructure and mechanical properties of high-strength steel with 20 mm thickness used for wind ...
Xuelin Wang +3 more
doaj +1 more source
Hydrogen‐Assisted Fracture of Iron‐Based Fe–Ni–Al Alloys
Principal relations and fracture mechanisms of single‐phase and precipitate‐strengthened Fe–Ni–Al alloys subjected to prior electrochemical hydrogen charging are identified. The mechanisms of hydrogen effect on strength and microhardness are discussed, including hydrogen‐induced increase in microhardness and the role of hydrogen in fracture behavior ...
Nataliya Yadzhak +3 more
wiley +1 more source