Results 171 to 180 of about 41,071 (268)

Predictive computational framework to provide a digital twin for personalized cardiovascular medicine. [PDF]

open access: yesCommun Med (Lond)
Lyu M   +7 more
europepmc   +1 more source

Influence of Heat Treatment on Microstructure and Mechanical Properties at Elevated Temperatures of Nonweldable Ni‐Based Alloy Printed by Fused Filament Fabrication

open access: yesAdvanced Engineering Materials, EarlyView.
The fused filament‐fabricated MAR‐M247 alloy without hot isostatic pressing shows the lowest porosity of 4%. Heat treatment at 1220 °C produces coarse precipitates and carbides. Specimens heat‐treated at 1220 °C exhibit higher tensile strength (683 MPa) and elongation (10%) at room temperature.
Haneen Daoud   +7 more
wiley   +1 more source

Energy Distribution during Resonant Acoustic Mixing. [PDF]

open access: yesACS Omega
Silverstein PD   +2 more
europepmc   +1 more source

On the Deformation Behavior of Metastable CrMnNi Steels Processed by Directed Energy Deposition in Different Temperature Regimes

open access: yesAdvanced Engineering Materials, EarlyView.
In the present study, metastable CrMnNi steels with varying chemical compositions and a concomitantly altered stacking fault energy are processed via directed energy deposition and afterwards tested via tensile tests at different temperatures. The present study shows the influence of the manufacturing process on the elemental deformation mechanisms for
Julia Richter   +8 more
wiley   +1 more source

Impact of aortic morphology on VA-ECMO performance: a combined statistical shape modeling and CFD approach. [PDF]

open access: yesFront Bioeng Biotechnol
Mazzoli M   +4 more
europepmc   +1 more source

Laser Metal Deposited Ti4822 Hollow Pipe: Experimental and Computational Modelling Study

open access: yesAdvanced Engineering Materials, EarlyView.
Laser metal deposition (LMD) of a crack‐free built Ti4822 alloys is challenging. This article reports outstanding characteristics of a hollow pipe that is built with LMD technology when a predicted, nontransformation substrate temperature of 800 °C is used.
Sadiq A. Raji   +5 more
wiley   +1 more source