Thermomechanical Fatigue and Creep–Fatigue Interaction of Inconel 718 Additively Manufactured by Laser Beam Powder Bed Fusion

open access: yesAdvanced Engineering Materials, EarlyView.
Thermomechanical fatigue tests of laser beam powder bed fusion (PBF‐LB) Inconel 718 show that the additively manufactured material reaches almost the lifetimes of conventionally‐rolled material under no‐dwell conditions. Introducing dwell times at the maximum temperature markedly reduces the lifetimes due to pronounced grain boundary sliding associated
Stefan Guth   +6 more
wiley   +1 more source

Fatigue Crack Initiation and Growth in Nanocrystalline Ni at Multiple Length‐Scales

open access: yesAdvanced Engineering Materials, EarlyView.
Overview of miniaturized in situ SEM fatigue setup and resultant fatigue crack growth data for nanocrystalline Ni. The presented study focuses on the analysis of fatigue crack growth rate (FCGR) in focused ion beam‐notched microcantilevers prepared from nanocrystalline (NC) Ni as a model material.
Igor Moravcik   +7 more
wiley   +1 more source

Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A

open access: yesAdvanced Engineering Materials, EarlyView.
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han   +5 more
wiley   +1 more source

Recycling of NiTi Shape Memory Alloys: Fundamental and Technological Aspects of a Vacuum Induction Melting Processing Route

open access: yesAdvanced Engineering Materials, EarlyView.
The present study investigates recycling of NiTi shape memory alloys via vacuum induction melting. An ingot was synthesized from elemental Ni and Ti and subjected to three subsequent remelting cycles. Remelting increases process durations and impurity levels and adversely affects microstructures and functional properties.
Sakia Sophia Noorzayee   +7 more
wiley   +1 more source

Current Status and Challenges in Data Collection for Aerospace Coatings Deposited by Plasma Spraying

open access: yesAdvanced Engineering Materials, EarlyView.
An innovative approach has been integrated into the GRENAT project to optimize plasma spraying and coating performance. Raw materials are accelerated and melted in the plasma generated by torches, creating coatings. Monitoring sensors collect process data which are combined with ex situ characterization data.
Lila Randriamananjara   +8 more
wiley   +1 more source

Molecular Dynamics Studies of Shape Memory Polymers: From Bead–Spring Models to Atomistic Simulations

open access: yesAdvanced Engineering Materials, EarlyView.
Coarse‐grained (left) and atomistic (right) models of the shape memory polymer ESTANE ETE 75DT3 are shown schematically. The two representations bridge molecular detail and mesoscopic description. Both models capture shape memory behavior, linking segmental mobility and conformational relaxation of anisotropic chains to macroscopic recovery, and ...
Fathollah Varnik
wiley   +1 more source

Experimental Characterization and Constitutive Modeling of the Effect of Prior Inelastic Strain on the Viscoplastic Behavior of AD730 at 700 °C

open access: yesAdvanced Engineering Materials, EarlyView.
This study shows that superalloys used in aircraft engine disks become much more prone to deformation at high temperatures if they have been strained during manufacturing. This effect increases with the level of prior strain but eventually reaches a limit.
Fabio Machado Alves da Fonseca   +9 more
wiley   +1 more source

Superlubricity and Corrosion Inhibition Properties of Solvate Ionic Liquids in Hybrid Carbon Fiber Reinforced Plastic–Steel Interfaces

open access: yesAdvanced Engineering Materials, EarlyView.
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...