Results 201 to 210 of about 1,892,709 (308)
Powder metal processing provides scalable advantages in nanoporous (np) metal development. Mechanical alloying is used to produce unique precursors for hybrid nanopore formation by oxide reduction and dealloying. As demonstrated in np Ag, this approach improves process efficiency while promoting smaller ligaments and larger pores, both of which are ...
Mark A. Atwater, Oliver A. Fowler
wiley +1 more source
Impact of Printing Angle and Layer Height on the Mechanical Strength of PLA Reinforced with Chopped Carbon Fibres Using FDM 3D Printing. [PDF]
Araque O +2 more
europepmc +1 more source
This study explores the lightweight potential of laser additive‐manufactured NiTi triply periodic minimal surface sheet lattices. It systematically investigates the effects of relative density and unit cell size on surface quality, deformation recovery, compression behavior, and energy absorption.
Haoming Mo +3 more
wiley +1 more source
Author Correction: Origin and tuning of bandgap in chiral phononic crystals
Wei Ding +8 more
doaj +1 more source
SWCNT/PEDOT:PSS/SA Composite Yarns with High Mechanical Strength and Flexibility via Wet Spinning for Thermoelectric Applications. [PDF]
Uchida K +5 more
europepmc +1 more source
The corrosion performance of AlSi7Mg and AlSi10Mg alloys produced through selective laser melting (SLM) was examined under compressive stress in a chloride environment. Electrochemical analyses, including open‐circuit potential (OCP), potentiodynamic polarization (CPP), and electrochemical impedance spectroscopy (EIS), were complemented by scanning ...
Femi John Akinfolarin +2 more
wiley +1 more source
Intratendinous Normal Saline Injection of Quadriceps and Patellar Tendon Allografts Does Not Reduce Mechanical Strength at Time Zero. [PDF]
Jacquez EA +8 more
europepmc +1 more source
This study demonstrates an efficient recycling route for out‐of‐spec AlSi10Mg atomized powders through compaction and arc remelting followed by suction casting. By correlating compaction load, cooling rate, and resulting microstructure, we show that intermediate pressures (50–80 kN) and rapid cooling refine dendrites, reduce porosity, and enhance ...
Mila Christy de Oliveira +4 more
wiley +1 more source
Degradation effects of reused PA12 powder in selective laser sintering on material characteristics, dimensional accuracy and mechanical strength. [PDF]
Vendittoli V +5 more
europepmc +1 more source