Results 151 to 160 of about 242,017 (306)
Intercritical annealing to achieve a positive strain-rate sensitivity of mechanical properties and suppression of macroscopic plastic instabilities in multi-phase medium-Mn steels. [PDF]
Benzing JT +5 more
europepmc +1 more source
This study investigates how tramp elements from increased scrap usage influence phase transformations in low‐alloyed steel. Combining dilatometry and microscopy reveal that tramp elements delay transformations, reduce critical cooling rates and increase hardenability.
Lukas Hatzenbichler +5 more
wiley +1 more source
The ability of the opportunistic yeast Candida albicans to acquire and maintain homeostatic levels of manganese (Mn), particularly in the metal-limited host environment, is an important determinant of its fitness.
Manon Henry +4 more
doaj +1 more source
Selenium was incorporated into a sol–gel‐derived bioactive glass to enable sustained therapeutic ion release. The selenium‐containing glass preserved bioactivity while selectively inducing cytotoxicity in osteosarcoma cells and maintaining osteoblastic viability.
Breno Rocha Barrioni +7 more
wiley +1 more source
Reversion kinetics during austenite reversion treatment (ART) significantly influence the microstructure and mechanical properties of medium Mn steels.
Min Seok Kim +3 more
doaj +1 more source
Numerical Modeling of Tank Cars Carrying Hazardous Materials With and Without Composite Metal Foam
Large‐scale puncture models consisting of hazardous materials (HAZMATs) tank car with protective steel–steel composite metal foam (S–S CMF) are solved numerically. Tank car plate with added 10.91–13.33 mm thick S–S CMF layer does not puncture. Protective S–S CMF absorbs impact energy, reduces plate deformation, and prevents shear bands formation ...
Aman Kaushik, Afsaneh Rabiei
wiley +1 more source
Microstructure Evolution of a VMnFeCoNi High‐Entropy Alloy After Synthesis, Swaging, and Annealing
The synthesis and processing (rotary swaging and annealing) of the novel VMnFeCoNi alloy is investigated, alongside the estimation of the grain size effect on hardness. Analysis of a wide grain size range of recrystallized microstructures (12–210 µm) reveals a low annealing twin density.
Aditya Srinivasan Tirunilai +6 more
wiley +1 more source
Tailoring Functional Properties of Ti–Ni–Cu Shape Memory Alloy Thin Films for MEMS Actuators
A comprehensive study of critical parameters required to develop well‐performing Ti–Ni–Cu thin film shape memory alloy microactuators is provided. Materials science and device integration aspects are integrated by addressing structural and physical relationships using complementary characterization techniques as well as a practical fabrication solution
Elaheh Akbarnejad +6 more
wiley +1 more source
Strong Interactions between Austenite and the Matrix of Medium-Mn Steel during Intercritical Annealing. [PDF]
Zhou T, Wang C, Wang C, Cao W, Chen Z.
europepmc +1 more source
Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han +5 more