Results 71 to 80 of about 5,347,175 (310)
Karl Popper and the Mechanisms of Hydrogen Embrittlement
Representation of the beginning of loss of ductility rather than embrittlement. Small concentrations of hydrogen in a diffusible form within iron are well‐established to harm the mechanical integrity of steels. There are theories that attempt to explain the pernicious role of hydrogen.
H. K. D. H. Bhadeshia
wiley +1 more source
Red Mud as an Additive in the Extrusion of Protein‐Based Porous Materials
This study explores the dual challenge of enhancing the properties of protein‐based foams produced from agricultural by‐products through the incorporation of red mud waste from alumina production.
Saga Holmström +5 more
doaj +1 more source
The EU steel industry accounts for a crude steel production of 140 Mt/y, provided by the integrated (57%) and electric (43%) routes, which respectively require up to 6.0 and 0.6 MWh/tCrudeSteel of energy input, and emits on average 1.85 and 0.4 tCO2 ...
Marco Simoni +10 more
doaj +1 more source
Building machine‐readable vocabularies for materials science is slow, expert‐driven work. This study benchmarks 13 large language models on two of its first steps: finding candidate terms in engineering articles and deciding where they belong in a class hierarchy.
Thomas Bjarsch +3 more
wiley +1 more source
Creep‐Induced Microstructural Evolution in an A2‐B2 Superalloy
A 27.3Ta‐27.3Mo‐27.3Ti‐8Cr‐10Al (at.%) refractory high‐entropy alloy with precipitation‐strengthened A2‐B2 microstructure was studied by creep tests at 1030°C, which demonstrate a transition in deformation mechanisms in the range of 100–150 MPa applied stress. This is associated with changes in dislocation–precipitate interactions. Relevant deformation
Liu Yang +10 more
wiley +1 more source
Aiming at the high value-added utilization of coal fly ash (CFA), the performance and reaction mechanism of key metals in asymmetric electrochemical recovery were explored.
Xuan LI +8 more
doaj +1 more source
Do not let thermal drift and instrument artifacts deceive high‐temperature nanoindentation results. We compare classical Oliver–Pharr and automatic image recognition analyses across steels and a Ni alloy to quantify these effects. Accounting for artifacts reveals systematic softening with temperature, while Cr and Ni additions boost resistance ...
Velislava Yonkova +2 more
wiley +1 more source
Assessing the Potential of Heterotrophic Bioleaching to Extract Metals from Mafic Tailings
Mafic mine tailings are highly resistant to bioleaching due to their silicate-rich composition, low sulfide content, and strong buffering capacity. This study aimed to assess the potential use of heterotrophic bioleaching to promote the release of metals
Kamalpreet Kaur Brar +2 more
doaj +1 more source
The present study investigates recycling of NiTi shape memory alloys via vacuum induction melting. An ingot was synthesized from elemental Ni and Ti and subjected to three subsequent remelting cycles. Remelting increases process durations and impurity levels and adversely affects microstructures and functional properties.
Sakia Sophia Noorzayee +7 more
wiley +1 more source
Pyrometallurgical Process to Recover Lead and Silver from Zinc Leaching Residue
During the roasting, leaching, and electrodeposition of zinc ores, lead–silver residues are produced. These residues contain valuable metals (Pb, Zn, and Ag) and toxic metals (Cd and As).
Cancio Jiménez-Lugos +7 more
doaj +1 more source

