Results 11 to 20 of about 11,703 (260)
Usually the element of real structures is subject of the mixed mode loadings. This fact can be explained by the elements geometry and the loading orientations.
Absi J., Dubois F., Pop O., Meite M.
doaj +1 more source
In this work, a series of intensive laboratory tests are conducted to measure the material constituents, mechanical properties, and to examine macro-micro-failure modes of various types of rocks from tight gas reservoirs in the Da Qing oilfield in China.
Zhaoyi Liu +9 more
doaj +1 more source
Ⅰ-Ⅱ MIXED-MODE FRACTURE PROPERTY OF 2D-C/SIC COMPOSITES (MT)
In order to characterize the Ⅰ-Ⅱ mixed-mode fracture performance of 2D-C/SiC composites, Arcan butterfly specimens with unilateral cracks were used, and the mode-Ⅰ and mode-Ⅱ fracture shape factors of the specimen were calibrated through finite element ...
LIN JiangRong +2 more
doaj
On a separating method for mixed-modes crack growth in wood material using image analysis
Due to the complex wood anatomy and the loading orientation, the timber elements are subjected to a mixed-mode fracture. In these conditions, the crack tip advance is characterized by mixed-mode kinematics.
Pop O., Dubois F., Moutou Pitti R.
doaj +1 more source
Fracture Toughness of Reactive Powder Fibrous Concrete Composites under Pure and Mixed Modes (I/III)
Reactive Powder Concretes (RPC) are well known for their exceptional strength properties and durability properties. The use of Supplementary Cementitious Materials (SCM) is the best way to enhance the strength and durability characteristics of RPCs ...
Sreekumaran Sreenath +2 more
doaj +1 more source
Experimental Investigation on Hydraulic Fracture Morphology of Inter-Salt Shale Formation
The inter-salt shale in the Qianjiang formation of Jianghan Basin in China is characterized by multiple salt-shale bedding planes, various rock strength, and high heterogeneity of rock mechanics.
Xiaoyu Zhang +6 more
doaj +1 more source
Relationship between microstructure and fracture types in a UNS S32205 duplex stainless steel [PDF]
Duplex stainless steels are susceptible to the formation of sigma phase at high temperature which could potentially be responsible for catastrophic service failure of components.
Maria Victoria Biezma +2 more
doaj +3 more sources
Mixed-Mode Fracture of Ceramics [PDF]
The mixed-mode fracture behavior of ceramic materials is of importance for monolithic ceramics in order to predict the onset of fracture under generalized loading conditions and for ceramic composites to describe crack deflection toughening mechanisms.
openaire +1 more source
The effect of loading rate on fracture energy of asphalt mixture at intermediate temperatures and under different loading modes [PDF]
At intermediate service temperatures hot mix asphalt (HMA) concretely are subjected to different loading rates due to movement of vehicles which can significantly affect their mechanical characteristics and final service load.
M.R.M. Aliha +3 more
doaj +1 more source
Criterion for Mixed Mode Fracture in Wood [PDF]
The mixed mode fracture failure of eastern red spruce (Picea rubens) was investigated by means of single edge notch and center crack specimens with various crack inclinations in the tangential‐longitudinal plane with propagation in the longitudinal direction (i.e., TL system of crack propagation).
S. Mall +2 more
openaire +1 more source