Results 11 to 20 of about 6,588 (235)
The mode II interlaminar fracture toughness characteristics of flax/glass/epoxy hybrid laminates were experimentally and numerically examined. Three types of hybrid composites that are made of flax (F) and glass (G) and with different layup sequences (i ...
Wilfred Stephen Ekeoseye +3 more
doaj +1 more source
Interlaminar fracture toughness is an important parameter to characterize the delamination performance of carbon fiber-reinforced epoxy laminates. In this study, the mode-I fracture toughness of interlaminar interfaces with different local ply angles ...
Chen Liu +7 more
doaj +1 more source
To improve the interlaminar properties of carbon fiber reinforced polymer composites (CFRPs), a hybrid fiber mat (i-MBP-PCF) was prepared by in situ deposition of a multiwalled carbon nanotube buckypaper (i-MBP) on the surface of functionalized CF fabric
Yadong Wu +6 more
doaj +1 more source
An experimental investigation is performed to investigate the effect of post-processing heat treatment on the interfacial fracture toughness of bi-material additively manufactured semi-crystalline polymer composite.
Md Fazlay Rabbi, Vijaya Chalivendra
doaj +1 more source
Fracture Behaviors of CFRP Laminates in Mode I Interlaminar Fracture Toughness Testing.
Fracture behaviours in mode I delamination tests of CFRP(T300/2500)were studied at cross-head velocity V=0.005∼200 mm/min. In low velocity region, serrations due to repeated unstable fracture appear on load P-displacement δ curve, and they become conspicuous as V becomes smaller.
Taketoshi NOJIMA, Takayuki KUSAKA
openaire +3 more sources
Effects of stitching on delamination of satin weave carbon-epoxy laminates under mode I, mode II and mixed-mode I/II loadings [PDF]
The objective of the present study is to characterize the effect of modified chain stitching on the delamination growth under mixed-mode I/II loading conditions.
AJ Kinloch +22 more
core +3 more sources
A new attempt to use a bifunctional interleaf for developing a novel structure–function-integrated composite with simultaneously improved interlaminar fracture toughness and atomic oxygen resistance was studied.
Miaocai Guo
doaj +1 more source
Effect of delamination interface angle on Mode Ⅱ delamination behavior of CFRP laminates
Mode Ⅱ interlaminar fracture toughness is an indispensable mechanical performance parameter for damage tolerance design of composite structure. The domestic T300 composite end notched flexure (ENF) specimens with five different delamination interfaces ...
ZHAO Wei, WANG Ya-na, WANG Xiang
doaj +1 more source
Delivering interlaminar reinforcement in composites through electrospun nanofibres
Electrospun nonwoven veils comprising thermoplastic fibres (average diameter 400–600 nm) based on polysulfone (PSU), polyamide (PA-6,6), and polyetherimide (PEI) have been fabricated and used as interlaminar reinforcements in carbon fibre composites ...
T. R. Pozegic +5 more
doaj +1 more source
The artificial accelerated cyclic hygrothermal aging test was conducted on T700/TDE86 carbon fiber reinforced resin matrix composites, and the effects of different cyclic hygrothermal aging days on interlaminar fracture toughness of composites with open ...
XU Kailong +4 more
doaj +1 more source