Results 1 to 10 of about 9,931 (244)
Dynamic nanoindentation by instrumented nanoindentation and force microscopy: a comparative review [PDF]
Viscoelasticity is a complex yet important phenomenon that drives material response at different scales of time and space. Burgeoning interest in nanoscale dynamic material mechanics has driven, and been driven by two key techniques: instrumented ...
Sidney R. Cohen, Estelle Kalfon-Cohen
doaj +3 more sources
Analysis of Nanoindentation Test Results of Asphalt Mixture with Different Gradations
Nanoindentation has been applied in the field of asphalt mixtures, but, at the nano-scale, changes in the composition of the mixture and material properties can have a significant impact on the results.
Yunhong Yu +5 more
doaj +1 more source
This paper investigates the orientation-dependent characteristics of pure zinc under localized loading using nanoindentation experiments and crystal plasticity finite element (CPFEM) simulations.
Pham T. N. Nguyen +4 more
doaj +1 more source
The magnesium phosphate cement (MPC) is a carbon-free cementitious material, widely used in solidification of nuclear waste, heavy metals, and repair and reinforcement.
Yue Li, Guosheng Zhang, Zigeng Wang
doaj +1 more source
Ferrule-top nanoindenter: An optomechanical fiber sensor for nanoindentation [PDF]
Ferrule-top probes are self-aligned all-optical devices obtained by fabricating a cantilever on the top of a ferruled optical fiber. This approach has been proven to provide a new platform for the realization of small footprint atomic force microscopes (AFMs) that adapt well to utilization outside specialized laboratories [D. Chavan et al., Rev.
Chavan, D. +6 more
openaire +2 more sources
INFLUENCING THE INDENTATION CURVES BY THE BLUNTNESS OF THE BERKOVICH INDENTER AT THE FEM MODELLING
The influence of the Berkovich indenter bluntness on the indentation curves at nanoindentation test of fused silica is determined by the FEM (finite element method) in this paper. The Berkovich indenter, which is mostly used for the nanoindentation test,
Jaroslav Kovář +2 more
doaj +1 more source
Review of Nanoindentation Size Effect: Experiments and Atomistic Simulation
Nanoindentation is a well-stablished experiment to study the mechanical properties of materials at the small length scales of micro and nano. Unlike the conventional indentation experiments, the nanoindentation response of the material depends on the ...
George Z. Voyiadjis +1 more
doaj +1 more source
Calibration of a Constitutive Model from Tension and Nanoindentation for Lead-Free Solder
It is challenging to evaluate constitutive behaviour by using conventional uniaxial tests for materials with limited sizes, considering the miniaturization trend of integrated circuits in electronic devices.
Xu Long +5 more
doaj +1 more source
Evaluating local strain rate sensitivity of titanium alloy using dynamic nanoindentation testing
Constant strain rate nanoindentation testing is useful for evaluating local strain rate sensitivity. In titanium alloys, the dwell fatigue at room temperature is a critical issue, and this phenomenon is known as relating to local strain rate sensitivity.
Yukimi Tanaka +2 more
doaj +1 more source
Nanoindentation of embedded particles
AbstractWe address the effect of elastic inhomogeneity on elastic modulus and hardness determinations made by depth-sensing indentations performed on individual particles embedded within a matrix of different elastic modulus. Finite element simulations and nanoindentation experiments are used to quantify the consequences of particle/matrix elastic ...
Slagter, Alejandra +2 more