Results 111 to 120 of about 2,010 (256)
Triboelectric charge generation at polymer‐metal interfaces arises from the interplay of intra‐ and inter transformation reactions of mechanochemically generated species, physical properties of polymers, environmental conditions. The direction and the magnitude of electron transfer between metal and polymer are dynamically governed by the relative ...
Sunay Dilara Ekim +4 more
wiley +1 more source
Thermally Induced Creep and Viscoelastic Behavior of Copper Micropillar Arrays
Copper micropillar arrays are fabricated by electrodeposition within through‐glass‐via, and their thermally induced time‐dependent deformation is quantified. Nanoindentation creep, EBSD, and TEM reveal a heat‐treatment‐driven transition between grain‐boundary‐mediated deformation and dislocation‐dominated creep, while Kelvin modeling captures ...
Miao Wang +14 more
wiley +1 more source
An Implanted Tooth That Can Feel
To endow the implanted tooth with masticatory perception, herein we demonstrate that a 3D‐printed piezoelectric‐core/robust‐sheath implanted tooth can rebuild the sensing feedback, serving as “mechanoreceptors” in converting the mechanical chewing force to electrical signals, and up to brain through surrounding alveolar nerve system.
Yaru Cao +13 more
wiley +1 more source
Bioinspired Microphase‐Engineered Binders for Silicon Anodes
Inspired by the tough exoskeleton of Phloeodes diabolicus, a bio‐based binder featuring LRA–click chemistry and hierarchical crosslinking forms well‐defined microphase‐separated structures that enable robust silicon anodes. This system promotes the formation of a LiF–rich, ultrathin SEI (∼17 nm) with high modulus and ionic conductivity, ensuring long ...
Lirong Tang +15 more
wiley +1 more source
Influence of Gas Flow Rate on the Deposition Rate on Stainless Steel 202 Substrates [PDF]
Solid thin films have been deposited on stainless steel 202 (SS 202) substrates at different flow rates of natural gas using a hot filament thermal chemical vapor deposition (CVD) reactor.
D.M. Nuruzzaman, M.A. Chowdhury
core
ABSTRACT Strain is a proven technique for modifying the bandgap and enhancing carrier mobility in 2D materials. Most current strain engineering techniques rely on the post‐growth transfer of these atomically thin materials from growth substrates to target surfaces, limiting their integration into nanoelectronics.
Berke Erbas +8 more
wiley +1 more source
Mechanism of Solid Solution‐Driven Texture Induced by Ag Doping in YBCO Superconductor
Ag‐doped YBCO with a designed concentration gradient is produced by dual‐material co‐extrusion and freeze‐drying. During annealing, Ag+ ions diffuse into Y123, substituting for Cu(1) and inducing c‐axis relaxation. This leads to the formation of [001]‐oriented YBCAO, creating a coherent interface that templates the textured growth of Y123. Consequently,
Fenyan Zhao +4 more
wiley +1 more source
This study utilizes programmable mechanical pressure as a therapeutic enhancer to establish a mechano‐chemotherapy strategy. Controlled pressure activates the mechanosensitive ion channel Piezo1 in bladder cancer, triggering a calcium ion cascade that transiently and reversibly amplifies membrane permeability to chemotherapeutics.
Minghai Ma +16 more
wiley +1 more source
Tumor metastasis results from complex interactions between cancer cells and mechanical microenvironments. We propose a “nucleus‐centered, cross‐stage mechanical signal decoding” model, highlighting how nuclear mechanosensors interpret forces at different stages.
Linqi Song +4 more
wiley +1 more source
Effects of carbon content and argon flow rate on the triboperformance of self-lubricating WS2/a-C sputtered coating [PDF]
Layered transition metal dichalcogenides (TMD) such as WS2 are materials well-known for their solid lubrication properties [1]. However, the lubricating property degrades through oxidation or moisture and it is also limited by its low hardness and low ...
Cao, Huatang +2 more
core +1 more source