Nanoindentation of Silicon

Materials Science Forum, 2008
The nanoindentation behaviours of single crystalline silicon samples has gained wide attention in recent years, because of the anomaly effects in the loading curve, caused by the pressure induced phase transformation of silicon. To further enlighten the phenomenon bulk, ion-implanted, single crystalline Si samples have been studied by nanoindentation ...
Péter M. Nagy   +3 more
openaire   +1 more source

Nanoindentation of polymers

Meccanica, 2011
This present work focuses on the surface characterization of reactor-thermoplastic-polyolefin copolymers (R-TPO) for automotive applications to deduce an appropriate parameter as a measure of the surface stickiness behavior. Therefore, nanoindentation experiments are performed and the well-known mechanical contact properties have been determined ...
Umut D. Cakmak   +2 more
openaire   +1 more source

Nanoscratching meets nanoindentation

Zeitschrift für Kristallographie - Crystalline Materials, 2016
AbstractA specimen of high-carbon nitrogen-doped steel has been synthesized to supplement previous studies on wootz-like steels. A comparison of different states of material as well as one of distinct methods of hardness testing has been performed. Electron microscopy of the specimens’ microstructure revealed nano-structuring similar to that observed ...
Irina P. Shakhverdova   +3 more
openaire   +1 more source

Nanoindentation of dental composites

Journal of Biomedical Materials Research Part B: Applied Biomaterials, 2005
AbstractThe intent of this project was to evaluate the elastic modulus and hardness of four composites with different fillers, a microfill, a hybrid, a dental resin cement, and a fiber filler, using nanoindentation. An indentation load of 0.001 N was used and 100 indents per specimen were taken. The elastic modulus measured for the Choice composite was
openaire   +2 more sources

Time-Dependent Nanoindentation

2004
In general, materials can resist deformation in a solid-like or viscous-like manner. Solid-like materials store energy under deformation, and upon removal of stress, returns to its original state. Viscous materials dissipate energy during deformation and upon removal of stress, remains in its deformed state.
openaire   +1 more source

Nanoindentation of coatings

Journal of Physics D: Applied Physics, 2005
A range of mechanical properties of a coating/substrate system may be obtained using indentation tests, and with the emergence of continuously recording indentation testing with nanometre penetration (often called nanoindentation) the mechanical properties of very thin coatings (
openaire   +1 more source

Nanoindentation of Polymers

2014
Small-scale polymers are increasingly being applied to a variety of fields, making it important to understand the behavior of polymers at small length scales. Indentation size effects (ISE) is the apparent increase in material-specific properties at very low indentation depths.
openaire   +1 more source

Nanoindentation Test Instruments

2002
Interest in nanoindentation has spawned a number of nanoindentation instruments that compete on a world market. Purchasers of such instruments are universities, private and government research organisations, and quality control laboratories. There is particular interest within the semiconductor industry that is concerned with the mechanical properties ...
openaire   +1 more source

Applications of Nanoindentation

2004
Nanoindentation finds a wide application. The test results provide information on the elastic modulus, hardness, strain-hardening, cracking, phase transformations, creep, fracture toughness, and energy absorption. Since the scale of deformation is very small, the technique is applicable to thin surface films and surface modified layers.
openaire   +1 more source