Isothermal Oxidation Behavior Characteristics of a Second Generation Ni-base Single Crystal Superalloy in Air at 1000 and 1100°C

open access: yesInternational Journal of Electrochemical Science, 2012
The isothermal oxidation behavior of a second generation Ni-base single crystal superalloy was investigated in air at 1000°C and 1100°C. The microstructures of the oxide morphology and the crosssection area of the specimens after oxidation were analyzed ...
Fahamsyah H. Latief   +3 more
doaj   +1 more source

Beneficial Effect of Pt and of Pre-Oxidation on the Oxidation Behaviour of an NiCoCrAlYTa Bond-Coating for Thermal Barrier Coating Systems [PDF]

open access: yes, 2011
The oxidation behaviour of a thermal barrier coating (TBC) system is a major concern as the growth of the thermally grown oxide (TGO) layer on the bondcoating creates stresses that greatly favour the thermal barrier spallation.
Monceau, Daniel   +4 more
core   +3 more sources

Effect of modification by Pt and manufacturing processes on the microstructure of two NiCoCrAlYTa bond coatings intended for thermal barrier system applications [PDF]

open access: yes, 2010
Few studies have already shown that Pt influences the diffusion of aluminium and therefore the microstructure of β-NiAl or γ-Ni/γ′-Ni3Al materials. Besides, several works have revealed that the addition of Pt to MCrAlY (M = Ni and/or Co) improves the ...
Lafont, Marie-Christine   +4 more
core   +1 more source

The Microstructural Degradation of Ni-Based Superalloys with Segregation under the Super-Gravity Condition

open access: yesMetals, 2023
The Ni-based superalloy is used as the turbine blade, which is subject to the coupling effect of temperature and super-gravity during service. As the Ni-based superalloys are difficult to become homogenous after using the solid solution heat treatment, a
Guo Yang   +7 more
doaj   +1 more source

Microstructural stability and lattice misfit characterization of nimonic 263 [PDF]

open access: yes, 2012
Nimonic 263 has been selected as a candidate header/piping material of advanced ultra-supercritical (A-USC) boilers for the next generation of fossil fuel power plant.
Barnard, Pete   +3 more
core   +1 more source

Kinetics of Grain Growth in 718 Ni-Base Superalloy

open access: yesArchives of Metallurgy and Materials, 2014
The Haynes® 718 Ni-base superalloy has been investigated by use of modern material characterization, metallographic and heat treatment equipment. Grain growth annealing experiments at temperatures in the range of 1050 – 1200 oC (1323–1473K) for time ...
Huda Z.   +4 more
doaj   +1 more source

Machine learning-assisted determination of material chemical compositions: a study case on Ni-base superalloy

open access: yesScience and Technology of Advanced Materials: Methods, 2023
The determination of chemical compositions of materials plays a paramount role in materials design and discovery. Optimization of such compositions can be a very expensive trial-and-error task, specially when the desired properties are very sensitive to ...
Sae Dieb   +3 more
doaj   +1 more source

Mechanisms of High Temperature Degradation of Thermal Barrier Coatings. [PDF]

open access: yes, 2009
Thermal barrier coatings (TBCs) are crucial for increasing the turbine inlet temperature (and hence efficiency) of gas turbine engines. The thesis describes PhD research aimed at improving understanding of the thermal cycling failure mechanisms of ...
Wu, Rudder T.C., Wu, Rudder T.C.
core   +1 more source

Slip analysis in a Ni-base superalloy [PDF]

open access: yesActa Materialia, 2005
A Ni-base superalloy single crystal with Gamma/Gamma' structure was tested at room temperature along the , and directions. Consistent with previously reported investigations, this alloy did not obey the Schmid law and the CRSS (critical resolved shear stress) was noticeably lower for the -oriented samples.
Materials Science and Engineering Department, University of Florida, P.O. Box 116400, Gainesville, FL 32611, USA ( host institution )   +3 more
openaire   +2 more sources

Role of tangential force coefficient on fretting fatigue life estimation of a single crystal Ni-base superalloy

open access: yesMechanical Engineering Journal, 2017
Fretting fatigue behavior of Ni-base superalloys used in gas turbine blades and disk assemblies have been investigated under ambient and high temperature conditions. A major emphasis was placed on the influence of experimentally measured tangential force
Balavenkatesh RENGARAJ   +2 more
doaj   +1 more source