Results 91 to 100 of about 2,044 (211)

Trustworthy Multimodal Attention Framework for Creep Rupture Life Prediction Under Data‐Scarce Conditions: A Case Study on IN718

open access: yesAdvanced Science, EarlyView.
An attention‐based multimodal deep learning framework is developed to predict the creep life of Ni‐based superalloys by fusing processing parameters with microstructural micrographs. The model achieves high accuracy (R2 = 0.92), aligns with metallurgical principles by capturing δ‐phase influence, and incorporates uncertainty quantification, offering a ...
Haopeng Lv   +10 more
wiley   +1 more source

Research progress in high-temperature high-entropy alloys

open access: yesJournal of Aeronautical Materials
High-temperature high-entropy alloys(HEAs)show potential to surpass traditional Ni-based alloys through multi-principal element synergy and microstructural regulation.
LI Haiyang, MA Zhaolong, CHENG Xingwang
doaj   +1 more source

Hydrogen‐Enhanced Stress Corrosion Cracking of Wire Arc Additive Manufactured Inconel 625 Superalloy in NaCl Solution: Mechanism of Synergistic Degradation

open access: yesMaterials and Corrosion, EarlyView.
Hydrogen‐enhanced SCC of WAAM Inconel 625 in 3.5 wt.% NaCl solution. Hydrogen charging reduces passive film stability (lower corrosion potential) and promotes pitting at Laves phase/matrix interfaces. Stress corrosion cracks propagate along Laves‐rich regions, leading to quasi‐cleavage brittle fracture.
Xu Zhang   +5 more
wiley   +1 more source

Study on the salt-corrosion and oxidation role mechanism of Ni-based single crystal superalloy in the long-term hot corrosion environment

open access: yesJournal of Materials Research and Technology
Hot corrosion is one of the key factors affecting the long-term service of Ni-based single crystal superalloys. In this paper, the long-term hot corrosion test of a second-generation Ni-based single crystal superalloy was carried out in a high ...
Y.Q. Yang   +5 more
doaj   +1 more source

Physics‐Informed Generative Machine Learning for Designing Crack‐Free γ′‐Strengthened Ni‐Based Superalloys for Laser Powder Bed Fusion

open access: yesMaterials Genome Engineering Advances, EarlyView.
This research proposes a physics‐informed generative machine learning framework to design SHA800, a crack‐free γ′‐strengthened nickel‐based superalloy for laser powder bed fusion, achieving a 43% γ′ volume fraction and 587 HV0.2 hardness. ABSTRACT Fabricating γ′‐strengthened nickel‐based superalloys via laser powder bed fusion (LPBF) faces significant ...
Kai Guo   +11 more
wiley   +1 more source

In-situ observation of Ni-Co based wrought superalloy high-temperature deformation: lattice rotation and grain boundary response

open access: yesMaterials Research Letters
The sensitivity of grain boundary (GB) cracks often limits the high-temperature plasticity of superalloys. The 750 ℃ tensile deformation of fine-grained Ni-Co based wrought superalloys was observed in situ using a scanning electron microscope (SEM ...