Results 161 to 170 of about 2,044 (211)
M<sub>x</sub>C<sub>y</sub>-Type Nanocarbide Crystallization in CrMnFeCoNi, CrMnFeCoNiV<sub>0.5</sub>, and CrMnFeCoNiMo<sub>0.5</sub> HEAs Manufactured Through Powder Metallurgy. [PDF]
Garcia AM +10 more
europepmc +1 more source
Effect of Deposit Chemistry on the Stress Corrosion Cracking Susceptibility of CMSX-10 at 550°C and 700°C. [PDF]
Martinez FD +6 more
europepmc +1 more source
Some of the next articles are maybe not open access.
Related searches:
Related searches:
Thermophysical Properties of Ni-Based Superalloys
2022Simulation of casting and joining processes and experimental planning are closely related to liquid metallic materials' thermophysical properties. Thermophysical properties datasets of Ni-based industrial alloys were analyzed through the application of experimental methods and theoretical models.
Novakovic R +4 more
openaire +2 more sources
Ni-based superalloys for turbine discs
JOM, 1999Superalloys have been developed for specific, specialized properties and applications. One of the main applications for nickel-based superalloys is gas-turbine-engine disc components for land-based power generation and aircraft propulsion. Turbine engines create harsh environments for materials due to the high operating temperatures and stress levels ...
David Furrer, Hans Fecht
openaire +1 more source
1999
Computer models for designing Ni-base superalloys have been developed. A mathematical model using regression equations based on microstructure and property databases has been established and successfully applied to alloy developments. Several types of Ni-base superalloys including new generation single crystal (SC) superalloys have been designed using ...
Hiroshi Harada, Hideyuki Murakami
openaire +1 more source
Computer models for designing Ni-base superalloys have been developed. A mathematical model using regression equations based on microstructure and property databases has been established and successfully applied to alloy developments. Several types of Ni-base superalloys including new generation single crystal (SC) superalloys have been designed using ...
Hiroshi Harada, Hideyuki Murakami
openaire +1 more source
A thermodynamic database for Ni‐base superalloys
Scandinavian Journal of Metallurgy, 2001A thermodynamic database has been developed for Ni‐base superalloys. Following the CALPHAD procedure, it is based on the assessment of thermodynamic behaviour of the relevant constituting sub‐systems of the complex system of interest. The current database contains 7 elements: Al, Co, Cr, Ni, Ti, W, Re.
N. Dupin, B. Sundman
openaire +1 more source
Hydrogen Embrittlement of Ni-Based Superalloys
CORROSION 1995, 1995Abstract The hydrogen embrittlement properties of some nickel based superalloys such as C-22, C-276, G-30 and Alloy 625 were studied. The alloys were studied for their susceptibility in annealed, cold worked and aged conditions. The degradation in mechanical properties were evaluated by slow strain rate testing.
Vimal H. Desai, Kirk Scammon
openaire +1 more source
Laser Cladding of Ni-Based Superalloys
2020Laser cladding of Ni-based superalloys has been studied extensively in the recent past owing to their combined properties of high strength and corrosion resistance at elevated temperatures, due to which they are finding wide applications in gas turbine engines, land-based power-generation gas turbines, nuclear and fossil fuel power plants, etc.
Gopinath Muvvala +2 more
openaire +2 more sources
Ageing kinetics of Ni-base superalloys
Materials at High Temperatures, 2016In the present work, the degradation of the γ/γ′ microstructure of single crystal Ni-base superalloy, CMSX-8, has been studied experimentally and computationally. Two microstructure evolution processes, referred to as rafting and coarsening, have been decoupled and investigated independently.
Sanam Gorgannejad +2 more