Results 21 to 30 of about 2,044 (211)

Stress corrosion of Ni-based superalloys [PDF]

open access: yesMaterials at High Temperatures, 2017
AbstractThe development of gas turbines to increase fuel efficiency is resulting in progressively higher operating temperatures in the under platform regions of the blades. These regions have traditionally been considered low risk areas. However, higher metal temperatures combined with stresses and the deposition of contaminants from the cooling air ...
Brooking, Laurie   +3 more
openaire   +2 more sources

Classification and microstructural stability of high generation single crystal Nickel-based superalloys

open access: yesZaštita Materijala, 2016
This paper presents a brief review on various types of single crystal Ni-based superalloys designed over the recent years. The design principles to achieve required mechanical properties and microstructural stability over the long time exposure to high ...
Roman Sowa   +2 more
doaj   +1 more source

On the origin of mosaicity in directionally solidified Ni-base superalloys [PDF]

open access: yesActa Materialia, 2021
This article addresses the formation of low angle grain boundaries which give rise to mosaicity, a phenomenon which has only recently received attention in the single crystal Ni-base superalloy field. In this work, post-mortem advanced microscopy characterisation techniques are employed to deduce the dendrite tip growth kinetics from transverse ...
Joel Strickland   +8 more
openaire   +1 more source

Electron and laser-based additive manufacturing of Ni-based superalloys: A review of heterogeneities in microstructure and mechanical properties

open access: yesMaterials & Design, 2022
The adaptation of additive manufacturing (AM) for Ni-based superalloys has gained significance in aerospace and power-generation industries due to the ability to fabricate complex, near-net-shape components on-demand and with minimal material waste ...
Nana Kwabena Adomako   +2 more
doaj   +1 more source

Microstructural evolution and dynamic recrystallization mechanism of a heavily-alloyed Ni-based superalloy during hot extrusion

open access: yesJournal of Materials Research and Technology, 2023
Direct hot forging of heavily-alloyed Ni-based superalloy castings usually ends up with severe cracking due to serious macro-segregation. To address this issue, we propose to use hot extrusion as the replacement technology to process this kind of ...
Xingyu Pan   +3 more
doaj   +1 more source

Energy-Assisted additive manufacturing for weldable and non-weldable Ni-based superalloys: a review

open access: yesVirtual and Physical Prototyping
Additive manufacturing (AM) of Ni-based superalloys has garnered significant attention for fabricating complex, high-performance components in aerospace, gas turbines, and other demanding applications, owing to its ability to achieve intricate geometries
Junmyoung Jang   +7 more
doaj   +1 more source

Rapid estimation of γ' solvus temperature for composition design of Ni-based superalloy via physics-informed generative artificial intelligence

open access: yesJournal of Alloys and Metallurgical Systems
The exceptional high-temperature mechanical properties of Ni-based superalloys are mainly stemmed from the L12 γ' phase, therefore it is crucial to discover Ni-based superalloys with high γ' solvus temperatures.
Yunfei Ren   +5 more
doaj   +1 more source

Thermal stability of Ni-based superalloys fabricated through additive manufacturing: A review

open access: yesJournal of Materials Research and Technology
Additive manufacturing (AM) is a cutting-edge technique that builds parts by adding layers from a digital design and depositing materials selectively where required. AM is vital in industries like aerospace, healthcare, and automotive because of benefits
Hedayat Hamdi, Hamid Reza Abedi
doaj   +1 more source

The Ni3Al/Ni Interfacial Contribution to the Indentation Size Effect of Ni-Based Single-Crystal Superalloys

open access: yesSolids
Hardness decreases as indentation depth increases at both the nano- and micro-meter scales. By incorporating interfacial contributions, the indentation size effect can provide valuable information on the deformation behaviors of Ni-based single-crystal ...
Zhiwei Zhang   +4 more
doaj   +1 more source

Impact of the Co/Ni-Ratio on Microstructure, Thermophysical Properties and Creep Performance of Multi-Component γ′-Strengthened Superalloys

open access: yesCrystals, 2020
The Ni content is a crucial factor for the development of γ′-strengthened Co-based superalloys and some studies have systematically addressed its influence on various properties in model superalloys.
Christopher H. Zenk   +4 more
doaj   +1 more source