Results 51 to 60 of about 2,044 (211)
Processing maps are key to guiding the thermo-mechanical processing (TMP) of superalloys. However, traditional processing maps are incapable of delimiting failure, which is an essential factor to be concerned about during the TMP of superalloys ...
Zonglin Chi +10 more
doaj +1 more source
The temperature dependence of fatigue behavior in nickel‐based superalloys is investigated through high‐resolution measurements of plastic localization. While increasing temperature reduces localization and enhances fatigue performance in René 88DT, Inconel 718 exhibits a sharp degradation at intermediate temperature due to intensified slip ...
M. Calvat +5 more
wiley +1 more source
Creep‐Induced Microstructural Evolution in an A2‐B2 Superalloy
A 27.3Ta‐27.3Mo‐27.3Ti‐8Cr‐10Al (at.%) refractory high‐entropy alloy with precipitation‐strengthened A2‐B2 microstructure was studied by creep tests at 1030°C, which demonstrate a transition in deformation mechanisms in the range of 100–150 MPa applied stress. This is associated with changes in dislocation–precipitate interactions. Relevant deformation
Liu Yang +10 more
wiley +1 more source
The microstructures and tensile properties of the Ni–Co-based superalloys made by additive manufacturing (AM) were investigated. The results revealed that both normal and inverse Portevin-Le Châtelier (PLC) effects were observed in AM Ni–Co-based ...
Ling Tang +8 more
doaj +1 more source
This overview presents a comprehensive exploration of the research methods employed for the precise assessment of volume fraction and the detailed characterisation of the size, shape and distribution of γ’ phase precipitates within Ni-based superalloys ...
Szczotok Agnieszka
doaj +1 more source
Do not let thermal drift and instrument artifacts deceive high‐temperature nanoindentation results. We compare classical Oliver–Pharr and automatic image recognition analyses across steels and a Ni alloy to quantify these effects. Accounting for artifacts reveals systematic softening with temperature, while Cr and Ni additions boost resistance ...
Velislava Yonkova +2 more
wiley +1 more source
Creep Properties and Deformation Mechanism of Additively Manufactured NiAl‐CrMo Composites
Additively manufactured NiAl‐CrMo composites contain numerous interfaces and cell boundaries that control their creep response. At 700°C under high applied stress, creep is dominated by dislocation‐controlled power‐law mechanisms. At 800°C–900°C and lower stresses, creep is primarily diffusion‐controlled along cell boundaries.
Jan Vollhüter +9 more
wiley +1 more source
Kinetics and Mechanisms of γ′ Reprecipitation in a Ni-based Superalloy [PDF]
AbstractThe reprecipitation mechanisms and kinetics of γ′ particles during cooling from supersolvus and subsolvus temperatures were studied in AD730TM Ni-based superalloy using Differential Thermal Analysis (DTA). The evolution in the morphology and distribution of reprecipitated γ′ particles was investigated using Field Emission Gun Scanning Electron ...
Masoumi, F. +4 more
openaire +3 more sources
Current Status and Challenges in Data Collection for Aerospace Coatings Deposited by Plasma Spraying
An innovative approach has been integrated into the GRENAT project to optimize plasma spraying and coating performance. Raw materials are accelerated and melted in the plasma generated by torches, creating coatings. Monitoring sensors collect process data which are combined with ex situ characterization data.
Lila Randriamananjara +8 more
wiley +1 more source
In Situ Micromechanical Study of Bimodal γ′–γ″ Precipitate Assemblies in Ni–Cr–Al–Nb Superalloy
A Ni–Cr–Al–Nb superalloy with a bimodal γ′–γ″ precipitate distribution is developed. Composite precipitate assemblies form through heterogeneous nucleation, effectively impeding dislocation motion. Micropillar compression reveals high strength at room and elevated temperatures, governed by precipitate shearing, with coupled faulting mechanisms ...
Ujjval Bansal +4 more
wiley +1 more source