Results 71 to 80 of about 23,475,186 (175)

Microstructural Material Analysis of Superalloy Inconel 792-5A after High Temperature Exposition

open access: yesCommunications, 2009
Aerospace industry often uses nickel superalloys for blades of jet engine turbines. The reason is that this material can satisfy numerous extreme requirements, such e.g. strength even at very high temperatures, resistance to fatigue damage, resistance to
Zdenek Jonsta   +2 more
doaj   +1 more source

In‐Situ Construction of Multi‐Scale Heterogeneous Structures in L‐DED IN718 Coatings via WMoTaNb Incorporation for Enhanced Strength‐Toughness Synergy

open access: yesRare Metals, Volume 45, Issue 10, October 2026.
ABSTRACT To improve the strength–toughness balance of IN718, and alleviate the brittleness commonly associated with refractory high‐entropy alloys, this study proposes a novel strategy to fabricate defect‐free IN718/WMoTaNb heterogeneous multiprincipal element alloy coatings via laser‐directed energy deposition.
Zhao Wang   +7 more
wiley   +1 more source

Effects of Cooling Rate on the Solidification and Microstructure of Nickel-Based Superalloy GTD222

open access: yes, 2019
In this work, the microstructure and solidification behavior of nickel-based superalloy GTD222 at different cooling rates are studied. The solidification of the superalloy GTD222 proceeds as follows: L → L + γ, L → L + γ + MC, L ...
Zunjie Wei   +6 more
core   +1 more source

The Effects of Thermo-Mechanical Treatments on Microstructure and High-Temperature Mechanical Properties of a Nickel-Based Superalloy

open access: yesCrystals
The effects of thermo-mechanical treatment and different annealing temperatures on the microstructure and mechanical properties of a nickel-based superalloy were investigated by metallographic microscope, scanning electron microscope, and mechanical ...
Zihan Kang, Yaxing Ma, Qian Lei
doaj   +1 more source

Fatigue of a polycrystalline nickel based superalloy: numerical simulation and physical experiment

open access: yes, 2018
Thermo-mechanical fatigue of a polycrystalline nickel based superalloy was studied by numerical simulation and physical experiment in order to understand effects of temperature, applied stress, and processing residual stress on microstructure ...
Liu, Yahui   +2 more
core   +2 more sources

Improved high-temperature-strength nickel-base superalloy [PDF]

open access: yes, 1969
Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the strength of the strongest available cast nickel-base alloys. It is not subject to the formation of embrittling phases upon long time exposure at intermediate
Waters, W. J., Freche, J. C.
core  

Creep-feed grinding of nickel-based superalloy GH4169 spline using micro-crystalline alumina wheels

open access: yesJin'gangshi yu moliao moju gongcheng, 2016
Nickel-based superalloy GH4169,as a typical difficult-to-cut material,has been widely used in aero-engine components.The micro-crystalline alumina wheel is becoming popular in grinding aeroengine materials due to its excellent performance of self ...
HE Jian   +3 more
doaj  

Progress in research and applications of additively manufactured nickel-based superalloy in aero-engines and gas turbines

open access: yesJournal of Aeronautical Materials
Nickel-based superalloy is an essential material to prepare hot-end components in aero-engines and gas turbines,due to its excellent mechanical properties under high temperature.
WU Yu   +7 more
doaj   +1 more source

Measurement and discussion of low-temperature hot corrosion damage accumulation upon nickel-based superalloy rene 104

open access: yes, 2008
Measurement and discussion of low-temperature hot corrosion damage accumulation upon nickel-based superalloy rene ...
RG Buchheit (17302264)   +1 more
core  

Towards low-friction and wear-resistant plasma sintering dies via plasma surface co-alloying CM247 nickel alloy with V/Ag and N

open access: yesMATEC Web of Conferences, 2015
Nickel based superalloys have good oxidation and creep resistance and hence they can function under high mechanical stress and high temperatures. However, their undesirable tribological behaviour is the major technical barrier to the challenging high ...
Zhang Zhenxue   +5 more
doaj   +1 more source

Home - About - Disclaimer - Privacy