Metal injection molding (MIM) is a technology that can be used to produce net-shape parts while reducing material waste and manufacturing costs. In the aerospace industry, the application of MIM to nickel superalloys (NiSAs) has been restricted to non ...
Rayner, Addison
core
Grain Refinement of a Powder Nickel-Base Superalloy Using Hot Deformation and Slow-Cooling. [PDF]
Fan X, Guo Z, Wang X, Yang J, Zou J.
europepmc +1 more source
Effect of machining allowance on machining quality in honing nickel-base superalloy
For typical difficult-to-machine materials of nickel-base superalloy GH4169,honing experiments are carried out to study the hole surface roughness and cylindricity.Resultsshow that the surface roughness decreases gradually and tends to be stable as ...
DONG Hongliang +5 more
doaj
The Image Analyses Utilization at Nickel-base Superalloy Degradation Classification
During operational conditions of internal combustion turbines of turbojet engines, the impeller blades are stressed by load cycles which vary in time, temperature and stress.
Řičánková, Veronika
core
Elution strategies for recovery of nickel and cobalt from laterite tails through scavenging resin-in-pulp [PDF]
Ion exchange resin has been used to recover value metal in the uranium and gold industry through resin-in-pulp/leach and similar carbon-in-leach/pulp processes for decades.
Vaughan, James +5 more
core
Effect of Heat Treatment Process on Microstructure and Fatigue Behavior of a Nickel-Base Superalloy. [PDF]
Zhang P, Zhu Q, Chen G, Qin H, Wang C.
europepmc +1 more source
Recent Advances in Creep Modelling of the Nickel Base Superalloy, Alloy 720Li. [PDF]
Harrison W, Whittaker M, Williams S.
europepmc +1 more source
A molten salt metal-air electrolyzer for recycling superalloy. [PDF]
Chen X +11 more
europepmc +1 more source
Weldability Improvement of Additively Manufactured Nickel-Based Superalloy by Controlling W and Si Migration at Solidification Front. [PDF]
Ma R +9 more
europepmc +1 more source
The Laser Welding Research of Dissimilar Materials Between AlCoCrFeNi2.1 Eutectic High-Entropy Alloy and GH3030 Nickel-Based Alloy. [PDF]
Liu A +5 more
europepmc +1 more source