Results 221 to 230 of about 757,728 (303)
The Socioeconomic Impact of Long-Acting Injectable Buprenorphine. [PDF]
Rasche SE +4 more
europepmc +1 more source
Soft Mechanical‐Electrical Logic Using Liquid Metal‐Filled 3D‐Printed Architectures
We present 3D‐printed soft mechanical–electrical logic elements that use liquid metal–filled silicone tubes actuated by thermoplastic polyurethane/polylactic acid (TPU/PLA) architectures to produce Boolean operations. Complementary normally open and normally closed unit cells perform repeatable binary transitions and can be combined into more complex ...
Christoph Lehmann +2 more
wiley +1 more source
Optimization of radiation protection using diagnostic reference values: current approaches and future directions. [PDF]
Almén A.
europepmc +1 more source
Enhanced Strength and Corrosion Resistance of Ti‐13Nb‐12Ta‐10Zr‐4Sn Alloy by Aging Treatment
This work systematically investigates the effect of aging treatment on mechanical properties and corrosion behavior of vacuum arc‐melted Ti‐13Nb‐12Ta‐10Zr‐4Sn alloy. Owing to the increased α″ martensite, strength and corrosion resistance were significantly enhanced by aging treatment.
Yuhua Li +5 more
wiley +1 more source
Biological Photoprotection: A Review of its Mechanisms, Evidence, and Clinical Implications. [PDF]
Brown A +8 more
europepmc +1 more source
OVER CURRENT PROTECTION OF ELECTRIC CAR CHARGING STATION
openaire +1 more source
Graphene nanoplatelet (0.1 wt.%) reinforcement significantly enhances the performance of β Ti‐28Nb‐35.4Zr alloy. Grain refinement, reduced water contact angle, and improved surface characteristics promote osteoblast adhesion and complete surface coverage after 7 days.
Khurram Munir +5 more
wiley +1 more source
PTSD and CPTSD amongst parents subject to child protection court proceedings: observed rates and associated demographic and clinical covariates. [PDF]
Graham K, Short R, Facer-Irwin E.
europepmc +1 more source
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.