Investigation of Iron‐Aluminide‐Like Phase Composition in Complex Concentrated Fe32Cu12Ni11Ti16Al29 Alloy

open access: yesAdvanced Engineering Materials, EarlyView.
This work reveals the phase composition and quantitative morphology analysis of precipitation‐hardened Fe32Cu12Ni11Ti16Al29 complex‐concentrated alloy. The precipitates are shown to have a high coherency. Morphology transition between sphere, cuboidal, and elongated morphology is observed. Finally, the overaging behavior is captured using microhardness.
Rostyslav Nizinkovskyi   +4 more
wiley   +1 more source

Pioneer of Biomedical Optics: Brian C. Wilson. [PDF]

open access: yesJ Biomed Opt
Pogue BW   +5 more
europepmc   +1 more source

The Effect of Thickness, Build Orientation, and Loading Rate on the Tensile and Compressive Properties of Selective Laser Sintering Polyamide 12 Specimens

open access: yesAdvanced Engineering Materials, EarlyView.
This article examines how build orientation, thickness, and loading rate affect the tensile and compressive properties of LS‐manufactured polyamide 12 12 parts. Through over 120 experiments, it reveals strong ductility anisotropy in tension, minimal compressive sensitivity, and significant thickness and strain rate dependencies.
Andreas Psarros   +2 more
wiley   +1 more source

Laboratory‐Scale Procedure for Evaluating the Flux Efficiency on Melt Cleanliness and Tensile Properties of Recycled Aluminum Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
A laboratory‐scale procedure is developed to evaluate the efficiency of melt‐cleaning and drossing fluxes during aluminium alloy recycling, studying their effects on melt cleanliness and tensile properties of secondary foundry alloys. This work provides a practical tool for foundries and aluminium refiners to assess the efficiency of salt fluxes in ...
Veronica Milani, Giulio Timelli
wiley   +1 more source

Microstructural Evolution and Mechanical Property Degradation of Sn0.5Ag0.7Cu5Bi Solder Joints with High Indium Alloying

open access: yesAdvanced Engineering Materials, EarlyView.
This study identifies 12 wt% indium (In) as the optimal composition for Sn0.5Ag0.7Cu5Bi solder joints, achieving 87% ductile fracture and 81% suppression of intermetallic compound (IMC) growth versus 4 wt% In. High‐In alloys (15–17 wt%) show abnormal IMC thickening due to thermal activation.
Liuwei Wang   +11 more
wiley   +1 more source