Results 161 to 170 of about 25,486 (191)

Ordnungszustände im system polyamid‐6 und polyamid‐6, 6

Makromolekulare Chemie. Macromolecular Symposia, 1986
AbstractBlends of PA‐6 and PA‐6,6 were studied by DSC for different conditions of crystallization. All samples were characterized by x‐ray diffraction. From dilute solution the components crystallize in separate modifications. In the melt both components are compatible. PA‐6‐ and PA‐6,6‐segments are linked together.
Wolfgang Keil, Gundolf Trafara
openaire   +1 more source

Preparation and properties of polyamide 6/polypropylene–vermiculite nanocomposite/polyamide 6 alloys

Journal of Applied Polymer Science, 2002
AbstractPolypropylene–vermiculite nanocomposites can be achieved by simple melt mixing of maleic anhydride‐modified vermiculite with polypropylene. Maleic anhydride acts either as a compatibilizer for the polymeric matrix or as a swelling agent for the silicate.
S. C. Tjong, Y. Z. Meng, Y. Xu
openaire   +1 more source

Composite Polyamide 6/Polypyrrole Conductive Nanofibers

Macromolecular Rapid Communications, 2009
AbstractConductive Polyamide 6 (PA‐6) nanofibers were prepared by making a conductive polypyrrole coating obtained by a polymerization of pyrrole molecules directly on the fiber surface. A solution of PA‐6 added with ferric chloride in formic acid has been electrospun and the fibers obtained showed an average diameter of 260 nm with a smooth surface ...
F. Granato   +3 more
openaire   +2 more sources

Crystalline properties of injection molded polyamide-6 and polyamide-6/montmorillonite nanocomposites

Applied Clay Science, 2009
Abstract This paper presents a study of the crystalline properties of injection molded samples of polyamide-6 (PA6) and polyamide-6/montmorillonite nanocomposites (PA6 MMT). Processing conditions and tool temperature during injection molding affect the crystal structure and the crystallinity of the samples.
A YEBRARODRIGUEZ   +3 more
openaire   +1 more source

Axial fatigue behaviour of polyamide-6 and polyamide-6 nanocomposites at room temperature

Composites Science and Technology, 2008
Abstract Design against fatigue requires thorough understanding of the underlying fatigue mechanisms and factors influencing them. The objective of the present work is to study the effect of nanoclay addition on the temperature rise and modulus drop during cyclic loading in polyamide-6 and polyamide-6 base nanocomposite.
A. Ramkumar, R. Gnanamoorthy
openaire   +1 more source

Investigation of thermal degradation and flammability of polyamide‐6 and polyamide‐6 nanocomposites

Journal of Applied Polymer Science, 2007
AbstractIn this paper, polyamide‐6 and polyamide‐6 nanocomposites were prepared by direct melt intercalation technique. The thermal degradation behavior of both polyamide‐6 and polyamide‐6 clay nanocomposites has been studied. The apparent activation energy of the nanocomposites is almost the same with that of pure polymer under nitrogen, but the ...
Ruowen Zong   +4 more
openaire   +1 more source

Fusion bonding of maleic anhydride grafted polypropylene–polyamide 6 blends to polyamide 6

Polymer, 1998
Keywords: Fusion bonding ; blends ; semi-crystalline polymers Reference LTC-ARTICLE-1998-003doi:10.1016/S0032-3861(98)00092-5View record in Web of Science URL: http://www.sciencedirect.com/science/journal/00323861 Record created on 2006-06-26, modified on 2016-08 ...
Jacques-Eric Bidaux   +4 more
openaire   +1 more source

Polyamide 6-6

Opérations unitaires. Génie de la réaction chimique, 1997
Cet article decrit la fabrication du polyamide 6-6 dans le cadre de son application dans le domaine des thermoplastiques techniques, le domaine d’application textile n’etant aborde que superficiellement. Ne sera traite que le procede de polycondensation de l’ adipate d’hexamethylenediamine (appele aussi Sel Nylon 6-6 ) en solution aqueuse par la ...
openaire   +1 more source