Results 101 to 110 of about 4,349 (291)
In NMR spectroscopy, samples are usually dissolved in deuterated solvents to avoid overlap of small analyte signals with large, protonated solvent signals.
Johanna Tratz +2 more
doaj +1 more source
Elongational viscosity of LDPEs and polystyrenes using entrance loss data
For two low-density polyethylenes and two polystyrenes, axisymmetric and planar elongational viscosities are estimated using entrance loss data from capillary and slit rheometers, respectively.
Koppi, K. A. +4 more
core +1 more source
Sustainable and Multifunctional Natural Macromolecular Polymers for Aqueous Zn Metal Batteries
We comprehensively review the structure‐function relationships and regulatory mechanism of natural macromolecular polymers in stabilizing zinc anodes at the microscopic and mesoscopic scales. The interactions among polymer structures, optimization strategies, and regulatory mechanisms are discussed systematically summarizing recent related research ...
Yunuo Shi +13 more
wiley +1 more source
Viscosity–temperature relationships for linear and 12‐arm star polystyrenes in dilute solution
The actual viscosities (cP) of dilute solutions of linear and 12‐arm star polystyrenes were measured in benzene, a good solvent, and cyclohexane, a poor to moderate solvent, as a function of temperature. The equations of Moore, previously established for
Mays, J.W. +3 more
core +1 more source
Rationale The ionization of polystyrenes in matrix-assisted laser desorption/ionization mass spectrometry (MALDI-MS) is typically achieved by the use of silver salts. Since silver salts can cause severe problems, such as cluster formation, fragmentation
Steinhoff, R.F. +13 more
core +1 more source
Micro‐topographical cues applied through temporally controlled microscale confinement improve the reproducibility, spatial organization, and neurosensory‐associated features of pluripotent stem cell‐derived inner ear organoids. Integration with a vascularized organoid platform further enables controlled investigation of vascular‐epithelial interactions
Harshita Sharma +15 more
wiley +1 more source
THERMAL STUDIES OF METAL POLYSTYRENES .4.
The thermal stability of metal polystyrene was determined by thermogravimetric analyses (TGA) from 25 to 250-degrees-C under nitrogen flow.The kinetic data obtained by TGA show that the thermostability of these polymers decreases in the following order ...
CARDENAS, G, RETAMAL, C, TAGLE, LH
core
Thermal degradation of phosphonated polystyrenes. Part 1: Chain and condensation
Polystyrenes substituted with chloromethoxyphosphonated groups at chain ends undergo a condensation reaction at a relatively low temperature (ca. 200°C) prior to extensive degradation of the polymeric chain (280-430°C).
Camino, Giovanni +12 more
core +1 more source
Adsorption‐Engineered Hydrocarbon Ionomers for Durable Proton‐Exchange Membrane Fuel Cells
Hydrocarbon ionomers suffer from oxidation‐driven interfacial degradation in PEM fuel cell cathodes, leading to catalyst instability. Here, adsorption‐engineered poly(fluorene) ionomers decouple interfacial anchoring from oxidative degradation, enabling strong catalyst–ionomer interactions while resisting electrochemical oxidation.
Heemin Park +14 more
wiley +1 more source
Polyphenol‐Inspired Materials for Agricultural Applications
This review outlines the use of polyphenol‐inspired materials for sustainable agriculture, highlighting their molecular design, interfacial assembly, structure–property relationships, and prospects toward precision agriculture, climate resilience, ecosystem protection, and circular bioeconomy strategies.
Haofu Liu +8 more
wiley +1 more source