Development of Sustainable MgO–C Refractories Using MgO–C Recyclates and a Novel Eco‐Friendly Fructose–Tannin Binder Crosslinked With Citric Acid

open access: yesAdvanced Engineering Materials, EarlyView.
This study develops sustainable MgO–C refractories using recycled materials and eco‐friendly fructose–tannin binders. The enhanced performance of citric acid as a cross‐linker and functional additives on mechanical and thermomechanical properties was examined. Characterization included strength tests, immersion trials, and microstructural and inclusion
Dinesh K. Gunasekar   +7 more
wiley   +1 more source

Creating Ti–Fe α/β Alloys by Diffusion‐Driven Solid‐State Processing

open access: yesAdvanced Engineering Materials, EarlyView.
This study proposes making alloys containing fast diffusing elements that are difficult to produce by ingot metallurgy, by diffusion‐driven solid‐state HIP processing of elemental powders and low‐temperature homogenisation. Here, novel Fe‐Ti α–β alloys are formed having fine α–β lamellae, a small β prior grain size without significant intermetallics ...
Jiaqi Xu   +10 more
wiley   +1 more source

Incorporation of Selenium into Sol–Gel‐Derived Bioactive Glass: Influence on Glass Structure, Bioactivity, and its Selective Cytotoxicity

open access: yesAdvanced Engineering Materials, EarlyView.
Selenium was incorporated into a sol–gel‐derived bioactive glass to enable sustained therapeutic ion release. The selenium‐containing glass preserved bioactivity while selectively inducing cytotoxicity in osteosarcoma cells and maintaining osteoblastic viability.
Breno Rocha Barrioni   +7 more
wiley   +1 more source

Numerical Modeling of Tank Cars Carrying Hazardous Materials With and Without Composite Metal Foam

open access: yesAdvanced Engineering Materials, EarlyView.
Large‐scale puncture models consisting of hazardous materials (HAZMATs) tank car with protective steel–steel composite metal foam (S–S CMF) are solved numerically. Tank car plate with added 10.91–13.33 mm thick S–S CMF layer does not puncture. Protective S–S CMF absorbs impact energy, reduces plate deformation, and prevents shear bands formation ...
Aman Kaushik, Afsaneh Rabiei
wiley   +1 more source

Impact of Pre‐Oxidation Treatments on a Recycled MgO/Steel‐Composite as Carbon Free Anode in Aluminum‐Electrolysis Environments

open access: yesAdvanced Engineering Materials, EarlyView.
Cermets (60 vol.% AISI 316L stainless steel, 40 vol.% recycled MgO), intended for use in aluminum electrolysis, were pre‐oxidized in three furnaces with different heating technologies and subjected to a cryolite corrosion test. The different atmospheres influenced the formation of oxide layers, which in turn affected corrosion resistance and ...