Results 41 to 50 of about 75,293 (304)
It is planned that Mod.9Cr-1Mo steel will be used as the structural material for the steam generator of the demonstration fast reactor. Creep strength of welded joints of Mod.9Cr-1Mo steel is lower than that of base metal at high temperature and long ...
Hayato YAMASHITA +4 more
doaj +1 more source
How to Extend the Life of Die-Casting Tools [PDF]
The paper explores some possibilities of extending the life of die-casting tools for non-ferrous metals, particu-larly aluminium, magnesium, and their alloys. In the first part of the paper is shown theoretical background of the problem.
Tušek, J., Taljat, B., Klobčar, D.
doaj
Powder metal processing provides scalable advantages in nanoporous (np) metal development. Mechanical alloying is used to produce unique precursors for hybrid nanopore formation by oxide reduction and dealloying. As demonstrated in np Ag, this approach improves process efficiency while promoting smaller ligaments and larger pores, both of which are ...
Mark A. Atwater, Oliver A. Fowler
wiley +1 more source
Influence of Multiple Repair Welding on Microstructure and Properties of 06Cr19Ni10 Stainless Steel
Repair welding technology is widely used in the manufacturing and maintenance of rail transit equipment to repair welding defects. However, repair welding induces modifications in joint performance, and it is necessary to study the microstructure ...
Qimeng Liu +7 more
doaj +1 more source
Laser repair welding of molds with various pulse shapes [PDF]
Repair welding of cold-work tool steels with conventional methods is very difficult due to cracking during remelting or cladding and is generally performed with preheating.
M. Pleterski +4 more
doaj
Repairing an Implant Titanium Milled Framework using Laser Welding Technology: A Clinical Report [PDF]
The application of laser welding technology allows titanium to be welded predictably and precisely to achieve accurate fit of a milled framework. Laser energy results in localized heat production, thereby reducing thermal expansion.
Prasad, Soni, Monaco, Jr., Edward A.
core +1 more source
It is shown that laser ablation pretreatment under oxygen‐free conditions enables copper–aluminium bonding at significantly lower deformation degrees and improved properties compared to mechanical brushing. Laser ablation further increases interface contact area and induces favourable residual stress states and microstructural compatibility ...
Khemais Barienti +11 more
wiley +1 more source
High-strength type-B sleeve for pipeline girth weld repair and its key application technology
In recent years, the repair technology of type-B sleeves has been widely used for the hazard control of pipeline girth welds. However, the prominent problems such as the unreasonable geometrical dimension of sleeve and the delayed cracking of fillet weld
Xinwei ZHAO +8 more
doaj +1 more source
Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar +2 more
wiley +1 more source
OM, SEM, EBSD and a series of mechanical property tests were used to study the influence of different welding lengths on the original welded joints. The results show that the filler welding area is austenitic structure due to the introduction of nickel ...
Min Zhang +5 more
doaj +1 more source

