Results 181 to 190 of about 2,599,445 (286)
To support future alloy development a powder mixture is processed by laser additive manufacturing. The powder mixture containing Mo‐ and W‐rich tracers is processed by powder bed fusion using single and double laser exposure and by directed energy deposition which provides drastically enlarged melt pools.
Felix Großwendt +2 more
wiley +1 more source
The study investigates the influence of DED‐Arc/M versus casting on the microstructure and material properties of X40CrMoV5‐1 (AISI H13) hot‐work tool steel. DED‐Arc/M yields finer microstructures, superior mechanical strength, and ductility, but slightly reduced thermal conductivity.
Ulf Ziesing +4 more
wiley +1 more source
Laser powder bed fusion of JIS SKD61 tool steel is systematically optimized using a Taguchi design and ANOVA. Hatch spacing and layer thickness are identified as dominant parameters controlling surface roughness and tensile strength. Subsequent tempering at 600°C improves microstructural stability and mechanical performance, enabling high‐density SKD61
Masrurotin Masrurotin +4 more
wiley +1 more source
Prebending of 304L/Q345R cladded plates significantly alters the subsequent weld thermal cycle and modifies the local interfacial microstructure. Combined electron backscatter diffraction (EBSD) and microscopy analysis demonstrates that deformation twinning, martensitic transformation, and defect initiation are concentrated at the trimaterial junction,
Ali Fahem +2 more
wiley +1 more source
A double intercritical annealing strategy is proposed to tailor the multiphase microstructure and mechanical response of a medium‐Mn steel. The treatment produces an ultrafine mixture of ferrite, martensite and multiple austenite populations with graded thermal and mechanical stability, formed through austenite reversion and controlled retransformation.
Mattia Franceschi +3 more
wiley +1 more source
This work uses high‐temperature dilatometry to examine how the tramp elements Cu, Ni, and Sn affect the deformability of non‐metallic inclusions and matrix in quench‐and‐temper steel. Mg‐bearing inclusions deform less than Mg‐free ones. Copper lowers formability. Nickel increases deformability.
Julian Cejka +3 more
wiley +1 more source
Paint baking of resistance spot welded joints of 2.0 GPa warm‐stamped medium‐Mn steel activates low‐temperature tempering, forming fine cementite in the fusion zone and enhancing toughness. Crack propagation resistance increases, shifting the failure mode from partial interfacial to complete pullout, with peak load and energy absorption rising ...
Sunusi Marwana Manladan +8 more
wiley +1 more source
The high‐strain‐rate behavior of resistance spot‐welded DP800–DP1000 joints is investigated. Results show that microstructural gradients across BM–HAZ–FZ govern hardness, strain rate sensitivity, and failure modes. While strength increases with strain rate, energy absorption is controlled by ductility, with DP800–DP800 joints showing superior ...
Pankaj Shrivastava, Velaphi Msomi
wiley +1 more source
Tailored heat treatments transform additively manufactured high‐nitrogen martensitic Cr steel from austenitic as‐built condition to high‐hardness states. Isothermal bainitizing at 250°C generates an ultrafine nanostructure and achieves higher hardness than conventional hardening and tempering, highlighting a promising postprocessing route for laser ...