Results 81 to 90 of about 7,811,095 (239)
Analysis of Variation of Stress Intensity Factor of Oblique Semi-Elliptical Surface Crack Using Singular Integral Equation Method [PDF]
In this paper, a singular integral equation method is applied to calculate the variation of the stress intensity factor along the front of a 3-D oblique semi-elliptical surface crack.
40172796 +12 more
core +1 more source
Economical design with sufficient fracture resistance is of high importance in any offshore pipeline projects. Using an Engineering Critical Assessment (ECA), alternate acceptance criteria for pipeline girth weld inspection can significantly reduce the ...
Mohammad Hossein Sharifi +3 more
doaj
The finite element method (FEM) is commonly used is solving engineering problems including fatigue crack growth. The S-version FEM is an extended version of the FEM to predict fatigue crack growth.
M.S. Shaari +4 more
doaj +1 more source
The neonatal brain surface on cranial ultrasound: Developmental anatomy and clinical implications
Abstract Cranial ultrasound is the most widely used neuroimaging modality in neonatal intensive care and allows the cortical surface to be followed longitudinally at the bedside; yet, a clinically applicable framework for reading it is lacking. In this narrative review we describe six landmarks—the lateral fissure, insula, sulcus centralis, sulci ...
Gertjan Marissens +8 more
wiley +1 more source
Using 3D Digital Image Correlation (3D-DIC) to Measure CTOD in a Semi-Elliptical Surface Crack
The subsurface nature of Crack Tip Opening Displacement (CTOD) makes its direct measurement very difficult, if not impossible. During fracture toughness testing, CTOD is commonly calculated by applying a plastic hinge model using externally applied clip ...
Kaveh Samadian +2 more
doaj +1 more source
Unveiling the Impact of Lateral Crack Formation on Median Crack Extension During Wheel Cleaving
ABSTRACT Wheel cleaving is a technique used to break glass sheets for various applications, such as in windows and displays. Despite the widespread adoption of this technique in industrial settings, the mechanisms underlying crack formation remain unclear. In particular, studies focusing on lateral cracks, which are known to significantly influence the
Kentaro Imai +6 more
wiley +1 more source
Abstract Macropeplus is endemic to Brazil and found above 1000 m elevation in the Atlantic Forest and Cerrado. Until this work, the four recognised species M. dentatus, M. friburgensis, M. ligustrinus and M. schwackeanus were initially separated by morphology and geographical distribution, with allopatric ranges.
Danilo A. Zavatin +3 more
wiley +1 more source
Due to the uncertainties related to the flaw assessment parameters, such as flaw size, fracture toughness, loading spectrum and so on, the probability concept is preferred over deterministic one in flaw assessment.
Beom-Jun Kang, Jeong-Hwan Kim, Yooil Kim
doaj +1 more source
ABSTRACT The present study proposes a combined approach of infrared thermography and 3D XFEM numerical models for crack process investigation in mechanical components such as gears. Over the years, fatigue crack analysis based on energy dissipations in the form of heat generated during fatigue tests has been widely reported, although mainly limited to ...
Luca Corsaro +3 more
wiley +1 more source
In this paper, a singular integral equation method is applied to calculate the distribution of stress intensity factor along the crack front of a 3-D semi-elliptical surface crack.
野田, 尚昭, 三好, 伸介
core