A Study of Grain Selection in Two-Dimensional (2D) Grain Selectors during the Investment Casting of Single-Crystal Superalloy. [PDF]
Zhu X, Wang F, Ma D.
europepmc +1 more source
Constitutive Modeling of Superalloy Single Crystals and Directionally Solidified Materials [PDF]
A unified viscoplastic constitutive relation based on crystallographic slip theory was developed for the deformation analysis of nickel base face centered cubic superalloy single crystals at elevated temperature.
Jordan, E. H., Walker, K. P.
core +1 more source
Biaxial constitutive equation development [PDF]
In developing the constitutive equations an interdisciplinary approach is being pursued. Specifically, both metallurgical and continuum mechanics considerations are recognized in the formulation.
Jordan, E. H., Walker, K. P.
core +1 more source
Microstructural Degradation and Creep Property Damage of a Second-Generation Single Crystal Superalloy Caused by High Temperature Overheating. [PDF]
Guo X +5 more
europepmc +1 more source
Creep Behavior Characterization of Nickel-Based Single-Crystal Superalloy DD6 Thin-Walled Specimens Based on a 3D-DIC Method. [PDF]
Zhang Y, Hu J, Kang L, He Y, Xu W.
europepmc +1 more source
On Extracting Mechanical Properties from Nanoindentation at Temperatures up to 1000$^{\circ}$C
Alloyed MCrAlY bond coats, where M is usually cobalt and/or nickel, are essential parts of modern turbine blades, imparting environmental resistance while mediating thermal expansivity differences.
Gibson, James S. K. -L. +3 more
core +1 more source
Interfacial Reaction Mechanism between Ceramic Mould and Single Crystal Superalloy for Manufacturing Turbine Blade. [PDF]
Yao J +5 more
europepmc +1 more source
Effects of Post-Weld Heat Treatment on Microstructure and Mechanical Properties of the Brazed Joint of a Novel Fourth-Generation Nickel-Based Single Crystal Superalloy. [PDF]
Zhang Z +7 more
europepmc +1 more source
Calibration approach to electron probe microanalysis: A study with PWA-1480, a nickel base superalloy [PDF]
The utility of an indirect calibration approach in electron probe microanalysis is explored. The methodology developed is based on establishing a functional relationship between the uncorrected k-ratios and the corresponding concentrations obtained using
Terepka, F. M. +2 more
core +1 more source
The Interdiffusion Behavior of NiCoCrAlYHf Coating Deposited by Arc Ion Plating on Carburized Ni-Based Single Crystal Superalloy. [PDF]
Chen Z +5 more
europepmc +1 more source