Results 71 to 80 of about 10,456 (224)

Estimation of the engineering elastic constants of a directionally solidified superalloy for finite element structural analysis [PDF]

open access: yes
The temperature-dependent engineering elastic constants of a directionally solidified nickel-base superalloy were estimated from the single-crystal elastic constants of nickel and MAR-MOO2 superalloy by using Wells' method.
Abdul-Aziz, Ali, Kalluri, Sreeramesh
core   +1 more source

Microstructural stability and lattice misfit characterization of nimonic 263 [PDF]

open access: yes, 2012
Nimonic 263 has been selected as a candidate header/piping material of advanced ultra-supercritical (A-USC) boilers for the next generation of fossil fuel power plant.
Barnard, Pete   +3 more
core   +1 more source

Deformation‐Induced Formation of Stray Grains in Additive Manufacturing of Single Crystals

open access: yesAdvanced Science, Volume 13, Issue 25, 4 May 2026.
Stray grain formation severely limits the additive manufacturing of single‐crystal alloys. By integrating in situ synchrotron techniques, ex situ characterization, and multi‐scale multi‐physics modeling, the authors reveal that stray grains originate from dislocations at the solid‐liquid interface, rather than thermal supercooling in conventional ...
Dongsheng Zhang   +11 more
wiley   +1 more source

Study on the salt-corrosion and oxidation role mechanism of Ni-based single crystal superalloy in the long-term hot corrosion environment

open access: yesJournal of Materials Research and Technology
Hot corrosion is one of the key factors affecting the long-term service of Ni-based single crystal superalloys. In this paper, the long-term hot corrosion test of a second-generation Ni-based single crystal superalloy was carried out in a high ...
Y.Q. Yang   +5 more
doaj   +1 more source

Substitution of Ti by Nb in Maraging Steel: Effects on Strengthening Mechanisms and Crystallographic Behavior

open access: yessteel research international, Volume 97, Issue 5, Page 2672-2692, May 2026.
This work demonstrates that replacing Ti with Nb in maraging steel forms nanoscale Nb–Mo particles along boundaries, strengthening the alloy without relying on Ti phases. Heat‐treatment tuning promotes uniform crystal orientation and balanced grain boundaries, enabling strong yet ductile behavior.
Mohamad Masoumi   +14 more
wiley   +1 more source

Effects of Hold Time on the Elevated Temperature Fatigue Crack Growth Behavior of Alloy 247LC‐DS

open access: yesFatigue &Fracture of Engineering Materials &Structures, Volume 49, Issue 5, Page 1794-1808, May 2026.
ABSTRACT Creep–fatigue crack growth (CFCG) experiments were performed at 850°C and 950°C on nominally 12.70‐mm‐thick compact‐type specimens of alloy 247LC‐DS, a Ni‐base superalloy. The loading cycles consisted of trapezoidal waveforms with hold times of 2 and 20 min at the maximum force.
Zachary B. Towner   +5 more
wiley   +1 more source

Dendrite Structure Refinement and Mechanical Property Improvement of a Single-Crystal Superalloy

open access: yesMetals
In the present work, the effect of different casting processes on the microstructure and creep properties of the second-generation single-crystal superalloy DD419 was investigated.
Hongyuan Sun   +5 more
doaj   +1 more source

Influence of Surface Orientation on Oxidation Resistance of Ni-based Single Crystal Superalloy CM186LC at 1100°C in Air

open access: yesInternational Journal of Electrochemical Science, 2012
The influence of surface orientation on the oxidation resistance of Ni-based single crystal superalloy CM186LC at 1100°C in air was investigated. The specimens with (001) surface showed a higher oxidation rate value compared to the specimens with (011 ...
Fahamsyah H. Latief   +2 more
doaj   +1 more source

Investigation of Creep Properties of Ti‐43Al‐5V‐4Nb Alloy Considering Oxidation Effects Using Miniature Specimens

open access: yesFatigue &Fracture of Engineering Materials &Structures, Volume 49, Issue 5, Page 1742-1755, May 2026.
ABSTRACT In the present study, creep tests of a TiAl alloy were conducted using miniature specimens (d = 2 mm) under various conditions to investigate their creep properties at 760°C. The test results indicate that creep rupture time obtained using miniature specimens at identical applied stress levels increase with the order of test condition Ar gas ...
Lei He, Takamoto Itoh, Noritake Hiyoshi
wiley   +1 more source

Lifetime Prediction of Single Crystal Nickel-Based Superalloys

open access: yesApplied Sciences
Single crystal nickel-based superalloys are extensively used in turbine blade applications due to their superior creep resistance compared to their polycrystalline counterparts. With the high creep resistance, high cycle fatigue (HCF) and low cycle fatigue (LCF) become primary failure mechanisms for such applications.
Kasar, Ç   +3 more
openaire   +3 more sources