Results 101 to 110 of about 1,610 (249)
Effect of rare earth Ce on arc and droplet transfer behavior
Five types of rare earth electrodes were produced by adding different amounts of cerium iron alloy to the original formula of the A147 electrode coating.
Runping CAO+4 more
doaj +1 more source
Stabilization of Mn4+ in synthetic slags and identification of important slag forming phases [PDF]
The expected shortage of Li due to the strong increase in electromobility is an important issue for the recovery of Li from spent Li-ion batteries. One approach is pyrometallurgical processing, during which ignoble elements such as Li, Al and Mn enter the slag system.
arxiv
Acidic Corrosion Behavior of Slag-free Self-shielded Flux-cored Arc Welding Overlay
Dashuang Liu+4 more
openalex +2 more sources
Defects detection of GMAW process based on convolutional neural network algorithm. [PDF]
Li H, Ma Y, Duan M, Wang X, Che T.
europepmc +1 more source
The impact of the internal welding defects on the joint strength [PDF]
The paper looks at the impact of the internal welding defects on the strength of joints. The tension tests provided the values of the welded joint strength limits depending on the area of sporadic voids, slag intrusions and the field of discontinuities ...
Rimantas Didžiokas+2 more
doaj +1 more source
PEMANFAATAN SUBSTITUSI SLAG WELDING SAW SEBAGAI AGREGAT KASAR PADA BETON
Lilis Tiyani+2 more
openalex +2 more sources
In this of globalization is growing very rapidly advancing technology. As well as in shipyard industry is toshipbuilding process. Submerged Arch Welding (SAW) is as joint methode of ship construction.
Kiryanto Kiryanto, Eko Sasmito Hadi
doaj
The production of chromium manganese ferroalloys for the use in the development of alloying loads of welding consumables is presented. On the basis of variations in the proportions of the chromium and manganese minerals in the loads, different ...
Lorenzo Perdomo-González+3 more
doaj
The submerged arc welding (SAW) process is complex because multi-phase reactions occur simultaneously across a large temperature interval from 2500 °C in the arc cavity, down to the weld pool liquidus temperare at the slag-weld pool interface.
Theresa Coetsee+1 more
doaj