Results 231 to 240 of about 1,471,382 (303)

Scaling of Planar Sodium‐Nickel Chloride Battery Cells to 90 cm2 Active Area

open access: yesBatteries &Supercaps, Volume 8, Issue 3, March 2025.
Large planar Na β′′ alumina electrolytes are prepared by tape‐casting and die‐pressing. These ceramic electrolytes are used to prepare planar sodium‐nickel chloride cells with 90 cm2 active area, providing a high capacity of 7 Ah. Successful cell cycling is demonstrated at 300 °C at rates up to C/4 (20 mA cm−2) for a cumulative capacity of 3.6 Ah cm−2.
T. Lan   +10 more
wiley   +1 more source

Comparative Study of High Voltage Spinel∥Lithium Titanate Lithium‐ion Batteries in Ethylene Carbonate Free Electrolytes

open access: yesBatteries &Supercaps, Volume 8, Issue 3, March 2025.
FEC and sulfone‐based co‐solvents are investigated as EC‐free electrolytes for LNMO∥LTO cells. FEC‐containing electrolytes demonstrate enhanced electrochemical stability by stabilizing the CEI and SEI layers, mitigating transition metal migration. Conversely, sulfone electrolytes form thinner CEIs and thick, sulfur‐rich SEIs, which are less effective ...
Killian Stokes‐Rodriguez   +6 more
wiley   +1 more source

Modeling Acoustic Attenuation, Sound Velocity and Wave Propagation in Lithium‐Ion Batteries via a Transfer Matrix

open access: yesBatteries &Supercaps, Volume 8, Issue 3, March 2025.
“A simple 1D transfer matrix model of a battery is introduced and parametrized using harvested individual cell components at 0 % and 100 % SoC. This model allows for the calculation of group velocity and attenuation. The results of the model show good agreement with measured values, highlighting increased attenuation and group velocity at the ...
Simon Feiler   +3 more
wiley   +1 more source

“Dead Lithium” Formation and Mitigation Strategies in Anode‐Free Li‐Metal Batteries

open access: yesBatteries &Supercaps, Volume 8, Issue 3, March 2025.
Anode‐free lithium metal batteries, though promising due to their high energy density, face challenges from dead lithium formation. “Dead lithium”, disconnected from the anode, causes capacity loss, increased resistance, and safety risks. This review explores the origins of dead lithium, its impact on battery performance, and potential strategies for ...
Mozaffar Abdollahifar, Andrea Paolella
wiley   +1 more source