Additive Manufacturing of Alumina‐Reinforced Elastomers

open access: yesAdvanced Engineering Materials, EarlyView.
Vat‐photopolymerized elastomers reinforced with platelet‐shaped alumina exhibited preferential orientation, reduced porosity, and significantly enhanced mechanical performance. A 3 wt% platelet loading increased tensile strength from 12.4 to 45.7 MPa, highlighting the critical role of filler morphology in elastomeric VPP composites.
Majid Barzegar Keyvani   +6 more
wiley   +1 more source

Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi   +5 more
wiley   +1 more source

On the stability of a quasicrystal and its crystalline approximant in a system of hard disks with a soft corona [PDF]

open access: yes, 2015
Using computer simulations, we study the phase behavior of a model system of colloidal hard disks with a diameter σ and a soft corona of width 1.4σ. The particles interact with a hard core and a repulsive square-shoulder potential.
Pattabhiraman, H.   +8 more
core   +1 more source

Enhancing Fatigue Crack Growth Resistance in Heterostructured Aluminum Bimetals by Tailored Interface Design

open access: yesAdvanced Engineering Materials, EarlyView.
Different Al/Al bimetals with a single engineered interface reveal how mechanical mismatch governs fatigue crack growth under cyclic loading. Additionally, loading–unloading–reloading tests link the microyielding behavior to the fatigue crack growth resistance, while crack‐path analysis reveals toughening mechanisms at the interface, highlighting ...
Sebastian Vollath   +2 more
wiley   +1 more source

Evaluation of soft tissue thicknesses of facial midline landmarks before and after puberty

open access: yesمجله دانشکده دندانپزشکی اصفهان, 2011
Introduction: In recent years, proportions and harmony of orofacial soft tissues have gained great importance in orthodontics. The aim of this research was to evaluate soft tissue thickness changes of facial midline landmarks during growth in both ...
Soosan Sadeghian   +4 more
doaj  

Jungck type fixed point results for weakly compatible mappings in a rectangular soft metric space

open access: yesJournal of Inequalities and Applications, 2019
The main objectives of the current study are to explore and to express the proof of some common fixed point theorems by using commuting maps in rectangular soft metric spaces.
Simge Öztunç, Sedat Aslan
doaj   +1 more source

Distinct Microstructural Characteristic Lengths Defining Notch Fatigue Crack Initiation and Propagation, and Defect Tolerance in Advanced Steels

open access: yesAdvanced Engineering Materials, EarlyView.
Schematic representation of modes of microcrack nucleation, growth and temporary arrestment at different boundaries, with the criteria for crack propagation in three scenarios: (1) large notch, (2) defect/small sharp notch, and (3) long crack. This work revisits and integrates results on the fatigue behavior of advanced bainitic steels (in particular ...
Lucia Morales‐Rivas
wiley   +1 more source

Multilayer Self‐Limiting Electrospray Deposition via Stepped Voltage Bias

open access: yesAdvanced Engineering Materials, EarlyView.
Self‐limiting electrospray deposition (SLED) uses a high voltage to generate and deposit a charged payload on a target surface. The coating retains its charge, repelling newly arriving material. SLED thickness can be decreased by applying a secondary bias to the target.
Madhuri Deb   +3 more
wiley   +1 more source

Superlubricity and Corrosion Inhibition Properties of Solvate Ionic Liquids in Hybrid Carbon Fiber Reinforced Plastic–Steel Interfaces

open access: yesAdvanced Engineering Materials, EarlyView.
Solvate ionic liquids lubrication reduced the coefficient of friction by ∼60% compared to dry sliding, reaching steady‐state values as low as 0.04–0.05. Corrosion weight‐loss measurements in 1 M HCl further demonstrated significant inhibition behavior, with only 100 ppm of [Li(G3)][TFSI] (∼68.5 μL/L) reducing corrosion‐product weight loss by 63 ...
Sameh Dabees   +6 more
wiley   +1 more source

Home - About - Disclaimer - Privacy