Grain growth stagnation in fully dense nanocrystalline Y2O3 by spark plasma sintering. [PDF]

open access: yes, 2010
Nanocrystalline (nc) Y2O3 powders with 18nmcrystallite size were sintered using spark plasma sintering (SPS) at 1100 ◦C and 100MPa for different durations. Specimens with 98% density and 106±33nm mean grain size were formed after 20 min.
Estournès, Claude   +2 more
core   +1 more source

Mechanical Performance and Tribological Behavior of WC-ZrO2 Composites with Different Content of Graphene Oxide Fabricated by Spark Plasma Sintering

open access: yesSci
This paper presents research on the effects of the addition of various contents of graphene oxide and sintering temperature on the mechanical, tribological, and electrical characteristics of WC-ZrO2 composites.
Anton Smirnov   +6 more
doaj   +1 more source

Sintering and densification of nanocrystalline ceramic oxide powders: a review [PDF]

open access: yes, 2008
Observation of the unconventional properties and material behaviour expected in the nanometre grain size range necessitates the fabrication of fully dense bulk nanostructured ceramics.
Levin, M.   +3 more
core   +1 more source

Processing and Characterization of AlN–SiC Composites Obtained by Spark Plasma Sintering

open access: yesSci
In this paper, the dependence of the microstructure and properties on Spark Plasma Sintering modes of an AlN-35 β-SiC (wt.%) composite is investigated. It was found that the use of a heating rate of 100 °C/min during the sintering process of the AlN-35 β-
Tatiana N. Smetyukhova   +6 more
doaj   +1 more source

Electrophysical Properties of the Multiferroic BFN-Ferrite Composites Obtained by Spark Plasma Sintering and Classical Technology [PDF]

open access: yesArchives of Metallurgy and Materials, 2020
In the paper the multiferroic (ferroelectric-ferromagnetic) composites based on ferroelectromagnetic/ferroelectric (BaFe1/2Nb1/2O3 (BFN)) powder and ferrite powder (zinc-nickel ferrite) were obtained by two technological methods. In the composite samples
D. Bochenek, P. Niemiec, D. Brzezińska
doaj   +1 more source

Effects of dispersion surfactants on the properties of ceramic – carbon nanotube (CNT) nanocomposites [PDF]

open access: yes, 2014
Gum Arabic (GA), Sodium Dodecyl Sulfate (SDS) and their mixture were used for the dispersion of multi-walled carbon nanotubes (CNTs) in an alumina matrix. A good dispersion at low loadings (0.5-1 wt%) of CNTs in alumina was achieved by an ultrasonic bath
Inam, Fawad   +4 more
core   +1 more source

The Effect of Layer Thickness and Nozzle Diameter in Fused Deposition Modelling Printing on the Flexural Strength of Zirconia Ceramic Samples Produced by a Multistage Manufacturing Process

open access: yesCeramics
The process of creating ceramic items using fused deposition modelling (FDM) enables the creation of intricate shapes for a variety of purposes, including tooling and prototyping.
Anton Smirnov   +9 more
doaj   +1 more source

Dielectric behavior of spark plasma sintered BaTi0.7Zr0.3O3 relaxor ferroelectrics

open access: yesResults in Physics, 2019
In the present work we have studied the transport and dielectric behavior of BaTi0.7Zr0.3O3 (BTZ30) relaxor ferroelectrics prepared by spark plasma sintering.
Mohamad M. Ahmad   +5 more
doaj   +1 more source

Phase Composition, Structure and Properties of the Spark Plasma Sintered Ceramics Obtained from the Al12Mg17-B-Si Powder Mixtures

open access: yesNanomaterials, 2022
In this work, composite materials were obtained by spark plasma sintering of an Al12Mg17-B-Si powder mixture. The structure, phase composition, and mechanical properties of the obtained composites were studied.
Pavel Nikitin   +5 more
doaj   +1 more source

Influence of sintering temperature and pressure on crystallite size and lattice defect structure in nanocrystalline SiC [PDF]

open access: yes, 2007
Microstructure of sintered nanocrystalline SiC is studied by x-ray line profile analysis and transmission electron microscopy. The lattice defect structure and the crystallite size are determined as a function of pressure between 2 and 5.5 GPa for ...
T. Ungár   +11 more
core   +1 more source