Results 181 to 190 of about 17,583 (228)
Some of the next articles are maybe not open access.
Developments in superalloy castability and new applications for advanced superalloys
Materials Science and Technology, 2009Increasing emphasis is being paid to optimising castability of cast superalloys to absolutely minimise defects which impact casting yield and alloy performance and to improve structural weldability of weld repairable alloys. The objective is to maximise casting yield and quality and minimise any rectification costs.
K. Harris, J. B. Wahl
openaire +1 more source
2010
Abstract This chapter provides a brief overview of nickel-iron-base, cobalt-base, and nickel-base superalloys, discussing their basic metallurgy and defining characteristics.
openaire +1 more source
Abstract This chapter provides a brief overview of nickel-iron-base, cobalt-base, and nickel-base superalloys, discussing their basic metallurgy and defining characteristics.
openaire +1 more source
2002
Abstract This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms.
openaire +1 more source
Abstract This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms.
openaire +1 more source
1979
Melting of superalloys is the initial, and perhaps most important, step in the production of materials used in critical high-temperature applications. Increasing demand for high-quality superalloys with specific characteristics has resulted in various combinations of primary, melting, refining, and secondary remelting operations.
openaire +1 more source
Melting of superalloys is the initial, and perhaps most important, step in the production of materials used in critical high-temperature applications. Increasing demand for high-quality superalloys with specific characteristics has resulted in various combinations of primary, melting, refining, and secondary remelting operations.
openaire +1 more source
JOM, 2012
This topic concerns advances in superalloys, and is sponsored by the TMS High Temperature Alloys Committee. Near-term developments on nickel-base superalloys are presented, as well as longer-term considerations for new superalloys. The High Temperature Alloys Committee sponsored a very successful International Symposium on Superalloy 718 and ...
openaire +1 more source
This topic concerns advances in superalloys, and is sponsored by the TMS High Temperature Alloys Committee. Near-term developments on nickel-base superalloys are presented, as well as longer-term considerations for new superalloys. The High Temperature Alloys Committee sponsored a very successful International Symposium on Superalloy 718 and ...
openaire +1 more source