Results 211 to 220 of about 5,060,373 (292)
The thermal diffusivity of MgO‐C refractories is highly sensitive to sample preparation and processing procedures. In this article, the effects of coking sequence, machining conditions, structural inhomogeneity, and graphite coating application on measurements using laser flash apparatus are systematically investigated.
Luyao Pan +4 more
wiley +1 more source
It is shown that laser ablation pretreatment under oxygen‐free conditions enables copper–aluminium bonding at significantly lower deformation degrees and improved properties compared to mechanical brushing. Laser ablation further increases interface contact area and induces favourable residual stress states and microstructural compatibility ...
Khemais Barienti +11 more
wiley +1 more source
VN Thin Films via MOCVD Using a New Vanadium Precursor: Linking Growth Chemistry to Functional Surface Properties. [PDF]
Glauber JP +11 more
europepmc +1 more source
Low‐cycle fatigue damage in Mn–Mo–Ni reactor pressure vessel steel is examined using a combined electron backscatter diffraction and positron annihilation lifetime spectroscopy approach. The study correlates texture evolution, dislocation substructure development, and vacancy‐type defect formation across uniform, necked, and fracture regions, providing
Apu Sarkar +2 more
wiley +1 more source
Tuning Titanium Surface Properties via μPPEO for Improved Osseointegration and Cell Adhesion. [PDF]
Melo NZP +5 more
europepmc +1 more source
This study investigates the tribological response of 60NiTi alloy under dry, water‐lubricated and high‐temperature conditions. The alloy exhibits decreasing wear volume and friction with increasing temperature due to the formation of protective oxide layers. The work clarifies dominant wear mechanisms and demonstrates the suitability of 60NiTi for high‐
Anthony Onyebuchi Okoani +2 more
wiley +1 more source
Influence of Machining, Polishing, and Glazing on Surface Properties and Biological Performance of Zirconia and Lithium Disilicate Dental Ceramics. [PDF]
Cho Y +7 more
europepmc +1 more source
Stabilization of L‐PBF Ni50.7Ti49.3 under low‐cycle loading was investigated. Recoverable strain after cycling was dependent on the amount of applied load. Recovery ratio was 53.4% and 35.1% at intermediate and high load, respectively. The maximum total strain reached 10.3% at a high load of 1200 MPa.
Ondřej Červinek +5 more
wiley +1 more source
Brushing With Charcoal Toothpastes on the Surface Properties of a Giomer: A Comparative In-Vitro Study. [PDF]
Marchan S +2 more