The presented study focuses on the fracture behaviour of carbon‐bonded magnesia MgO–C refractories, where environmentally friendly fructose, collagen and lignin serve as temporary binding agents. The partial substitution of the source material with recycled MgO–C reduces the fracture resistance, which can be counteracted by the additional introduction ...
Marc Neumann +6 more
wiley +1 more source
On the evaluation of surface tension of biodiesel. [PDF]
Rezaei F +6 more
europepmc +1 more source
Effect of Laser Deoxidation on Adhesive‐Bonded Aluminum in an Oxygen‐Free Atmosphere
This study investigates laser ablation of aluminum under oxygen‐free conditions. The goal is to produce oxide‐free substrates that enable improved adhesive bonding with epoxy. Optimized laser parameters (90% overlap, 300 µJ) combined with oxide‐free substrates result in the highest tensile strength of the adhesive bond.
Sandra Gerland +5 more
wiley +1 more source
Quantifying surface tension of metastable aerosols via electrodeformation. [PDF]
Shahabadi V +6 more
europepmc +1 more source
Four‐point bending tests are conducted in an argon atmosphere on commercial MgO‐C brick grades with and without MgO‐C recyclate from room temperature up to 1300 °C. No detrimental effect of the MgO‐C recyclates on bending strength is found. Instead, a decisive influence of the total carbon content is observed, with lower total carbon contents ...
Alexander Schramm +5 more
wiley +1 more source
Curvature-Enhanced Superomniphobic Property for Minimizing Contact Time of Low-Surface-Tension Liquid. [PDF]
Ahn H +5 more
europepmc +1 more source
This study investigates thermo‐chemical processes during high‐temperature testing of two commercial MgO‐C brick grades, one containing 47.5 wt.% MgO‐C recyclate. Using ETV, DTA/TG‐MS, XRD, and SEM/EDS/EBSD, mechanisms such as carbothermal reduction of magnesia, impurity incorporation into the secondary MgO surface layer, and calcium‐rich phase ...
Alexander Schramm +6 more
wiley +1 more source